25-05-05The permeability of iron varies with temperature.
Not only does it change with temperature but iron has a non-linear permeability. It varies depending on magnetic field and previous magnetic state.
Which permeability are you interested in? Maximum permeability, initial permeability, permeability at saturation, etc.?