Latest threads in ⚗ Material Sciences show only best voted threads
Subject | Author | Posted | Replies | |
---|---|---|---|---|
|
shearing al
Hello Does anyone know the kind of forces needed to shear a 2mm thick sheet of aluminium ? Also any ideas on the same - for sandwiches of aluminium alloy layers with fibre reinforced composite in the...
—
|
17 years ago
|
— | |
|
Nitinol help
Hi: I need some information about Nitinol. A quick literature survey says that it can be sputtered. But, none of them give the source of the sputter target. Anyone know where I could order such a...
2
|
17 years ago
|
2 | |
|
How to creat Hrdrophobic ITO?
I am interesting in Highly hydrophobic ITO or FTO glass. (P.S. I am open for any suggetions
2
|
17 years ago
|
2 | |
|
metal forming dies
From where can I obtain steel forming dies that can attach to an Instron type machine and punch a shape into sheet metal, I just need simple shapes with some curvature Any advice is much appreciated...
—
|
17 years ago
|
— | |
|
piezoceramic
I am doing some researches about piezoceramic materials,but I can find no referance and site about how to provide the materials and mixture them. It would be so much appreciated if anyone help me.
—
|
17 years ago
|
— | |
|
Industry linked studentship Oxford
UNIVERSITY OF OXFORD Industry-Linked D. Phil. Research Studentship Condensed Matter Sub-department Clarendon Laboratory Parks Road Oxford OX1 3PU United Kingdom We are seeking a suitably qualified...
—
|
17 years ago
|
— | |
|
Stainless Steel 316 Bearing Interference
I have an application where we have an 1 5/8" SS 316 shaft oscillating thru 100 deg in a SS 316 bearing ( 1 " in length ) with marine grease. We are committed to 316 beacuse of corrosion issues. We...
2
|
17 years ago
|
2 | |
|
A new FBG device for dynamic monitoring
A new FBG device for dynamic monitoring TRICOM has completed Fiber Bragg Grating Dynamic Interrogator FBG-3000. It is the most advance high speed Interrogator for Fiber Bragg Grating sensing, the only...
—
|
17 years ago
|
— | |
|
PET data
Hi, Does anyone know any web site where I can find the DTA and the TGA graphs for PET thermoplastic? Regards, Edward
—
|
18 years ago
|
— | |
|
Alulife Aluminium
Hi all is there anyone who can give me some information about this new material used for house's paviment or for design works as chairs or tables? thanks Cerac
—
|
18 years ago
|
— | |
|
large aluminum discs?
I found this company that has large aluminum discs for sale- have different diameters and thicknesses at great prices.
—
|
18 years ago
|
— | |
|
electromigration in copper lines: role of texture and microstructure
I have read a few papers on the role of texture and grain size in electromigration MTTF. The most famous work on this is the Vaidya-Sinha equation which says MTTF depends on grain size & distribution...
1
|
18 years ago
|
1 | |
|
chitosan
hi am working on chitosan. i have some difficulty in purification of chitosan. when i precipate it dil NaOH solution it give my white color pulp like material which on drying become compressed and...
2
|
18 years ago
|
2 | |
|
solder for UHV
I am working on a system under UHV at very low temperature. Now I need to solder thermocouple wires to feedthrough (i.e. two copper pins sticking inside from one fo the vacuum port. I want to solder...
8
|
18 years ago
|
8 | |
|
Problems with dense phase conveying systems for alumina (scaling, fouling)
Hello, my name is Arne L=FCken and I am studying process engineering in Hamburg Germany. In line with my studies I am working on a research about the phenomena of scale formation which occurs while...
—
|
18 years ago
|
— |