I have notice when buying tool steel the smaller the quanity you buy the more expensive it gets
so I thought would it be possible to make my own in a crucible by mixing scrap stainless, mild steel and a measured amount of powdered graphite to up the carbon content
anyone got any idea if this could work?
TIA
George
Didn't find your answer? Ask the community — no account required.
I think there is a problem of what material we are refering to in thefirst...
I
Ian Stirling
Sure, once you've got the appropriate crucible, furnace, temperature controller, exact specs of the alloy you require and your ingredients, it's almost trivial.
J
Jon Grimm
almost trivial.
much like income taxes =)
E
Ed Huntress
Yes, and the idea is "no." They don't mix alloy steels that way. There is an order, and there are fluxes (some constituents are pellets coated like M&M's with fluxing and intersolute materials). They don't use scrap to make tool steel. There is a lot of metallurgical control required to make anything worthwhile.
Without remelt capabilities (electroslag or vacuum-arc remelt; don't even consider it), the quality you could produce would be so much lower than any European- or American-made tool steel that it wouldn't be worthwhile. You'd be competing with China at the junk end of the scale.
Sorry to sound so discouraging, but you're barking up the wrong tree. Why don't you consider getting a bunch of people together to buy in some quantity?
Ed Huntress
T
Ted Edwards
I make a lot of tools from old car/truck springs both leaf and coil. Easy to anneal, machine, grind, forge, harden and temper.
Ted
T
Tim Williams
But not necessarily not worth trying... Could do it the way they did in the 1700s - take mild steel bars (they used wrought iron), chop them up into 1/4" cubes, rods, whatever, bury in charcoal and heat for a few days to give a good thick case hardening on the stuff, then melt in a crucible furnace (yes you can melt steel with coal or charcoal). Hopefully the center will still be soft and mild, while the outer layer will be near cast iron in carbon content; when these melt together, you get something inbetween.
Begs the question, why didn't they just take wrought and a little cast iron, melt the one and pour the other into it. Maybe they couldn't get it quite hot enough to melt the nearly-pure steel. (What a difference just 100°F makes!) Or they didn't make the connection.. but this was still going on during the 19th century when they had the chemistry. And then Bessemer came along...
Tim
-- "That's for the courts to decide." - Homer Simpson Website @
formatting link
E
Ed Huntress
If the idea is to recreate the processes that produced the tool steels of the 19th century, then have at it. If the idea is to save money by making your own tool steel, and if you're comparing it with a modern tool steel, then it ain't gonna happen.
Those experiments are fun and satisfying. But I got the impression that the poster was just trying to save money.
Ed Huntress
H
Harold & Susan Vordos
Great idea, but far from modern high quality tool steel. The tool steels of today are not necessarily just carbon steel and don't necessarily rely on the carbon cycle for hardness. There are tool steels that have no iron in their makeup.
Precipitation hardening steels are a good example of steels that don't exclusively rely on carbon for hardness. Are you familiar with Vasco-Max? Vasco-Max 350 is capable of tensile strength of 350,000 PSI. Try getting that out of carbon steel.
I agree with Ed, trying to duplicate super alloy tool steels of today in order to save a few bucks is insanity. Doing it for fun, on the other hand, would be an interesting experience, one that would give the experimenter tremendous respect for those that are making fine quality tool steels with reliable characteristics using modern technology and sophisticated equipment. Some things are best left to those with knowledge and proper tooling, particularly for analysis in process to control the end result.
That's my take on it, anyway.
Harold
L
Ljwebb11
If you are ordering from the tool supply houses, the price is extremely high. You can get a better price directly from the tool steel houses, but you need quantity. I bought 500lbs of A-2 last week for about 75 cents a pound. Some of the tool steel houses will sell remnants cheap. I try to keep at least a 1000lbs of tool steel on hand at all times. I have an aversion to paying full price and am always on the lookout for deals. Tough to find a deal on a small quantity.
I remember buying a length of S-7 hollow bar that had a shipping sticker from from McMaster-Carr on it. From Mc-M it would have cost $140. I paid $20 for it. You just gotta get out there and dig for the deals.
Les
G
Gary Coffman
No iron?
Gary
H
Harold & Susan Vordos
I offer you, for example, Haynes Stellite, which is iron free. It is comprised of chromium, cobalt and tungsten.
Harold
J
Jeffrey Lindemuth
I would submit then that it is not steel. Very useful material but not steel. Haynes Internation, the manufacture, never refers to it as steel on their history page:
formatting link
Good reading on this page. I never knew that Hastelloy was an acronym, that begame a word.
Jeff
W
Wayne Bengtsson
Are you sure it can be called "steel" if it doesnt have iron and some carbon in it?
J
jim rozen
Aside from the aforementioned 'mahogany pistons' I think the comment was more along the lines of, 'steel' is often defined as having iron as a constitutent. Stellite might be a perfectly fine cutting tool, but like the cemented carbides (tungsten, cobalt, carbon) it had no iron and as such might be excluded from the 'tool steel' designation on that basis alone.
The cemented carbides are not considered tool steel, so I would propose that stellite might also not be.
Jim
================================================== please reply to: JRR(zero) at yktvmv (dot) vnet (dot) ibm (dot) com ==================================================
E
Ed Huntress
Ah, terminology, terminology. Stellite isn't steel, Harold. It's a superalloy.
What's in a name? Anyway, it needs iron and carbon in it to be steel. Some superalloys contain iron, but they're mostly alloys of nickel, chromium, cobalt, etc.
Ed Huntress
H
Harold & Susan Vordos
Agreed. Not steel as such, but commonly used as tool steel before tungsten carbide became so popular. The point is that "tool steel" doesn't necessarily contain iron, no more than an iron found in a women's list of household tools does. I suggest that type of iron is made of aluminum.
I think that, for the most part, all of us know and understand that steel is an alloy of iron and carbon in which the carbon is dissolved in the iron, it is not found in a free state, such as it is in gray or ductile iron.
Harold
H
Harold & Susan Vordos
Carbon in SOLUTION, to be exact, not just carbon. Yep, I know that, just as you know that Stellite tool bits are commonly referred to as tool steel. You know, like aluminum irons. Makes no sense, but we still say it.
:-) Harold
J
jim rozen
So it's OK to call carbide inserts tool steel?
Of course not!
Jim
================================================== please reply to: JRR(zero) at yktvmv (dot) vnet (dot) ibm (dot) com ==================================================
E
Ed Huntress
In 30 years in the business, I've never heard of Stellite tool bits referred to as "tool steel." Jargon and terminology vary all over the industry, like the names of sunfish to fishermen, but that's one that's escaped me.
Usually, they just call it Stellite. In the aerospace industry, it's recognized as a superalloy.
Ed Huntress
H
Harold & Susan Vordos
I agree, and I've never encountered that, but I still hear the term iron when used for the device women used to use before women's lib.
Harold
H
Harold & Susan Vordos
Most likely because it has disappeared from the scene (in the way of toolbits, that is), thanks to carbide replacing it.
I have no quarrel with that, Ed, because it is rarely used as a cutting tool anymore, it makes more sense when you look at it that way. As you said, "Ah, terminology, terminology". I recognize that it is not steel, that was my point in posting what I did. Many of our terms are used improperly. This was an example. The way I see it, any die or cutting material is commonly referred to as "tool steel", including medium to high carbon steel.
Harold
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?
Ask the community — no account required
Report Content
You are reporting this content to the moderators. They will look at it
ASAP.