seeking good laser welding shop

Feb 13, 2008 0 Replies

I need to find someone with a laser welder to weld up 3 small and simple battery cases quickly. These are protoypes so I need a quick turn around time. Are any of you interested or can you recommend a good laser welding shop? I can send you the drawings in case you are interested. The detailed rfq is below:


Request for Quote rev 021208 720p



Subject: Laser weld battery case to provide hermetic seal



Contact: Doug Danielson Atlanta, Georgia 30312



404 667 4680 mobile snipped-for-privacy@hotmail.com

Summary: We need to obtain price and lead time quotations for laser welding a seam in a small stainless steel battery case to produce a hermetic seal. These are prototype assemblies so small order quantities (~3 assemblies) and quick turnaround time are expected.



Requirements: Battery components must be immersed in an argon atmosphere during welding Battery cells contain a thin film of lithium metal that will corrode if exposed to moisture Temperature of internal battery cells cannot exceed 150C Battery cells contain a thin film of lithium metal that will melt if heated above 150C Leak test battery after welding to confirm hermetic seal



Details: Please quote lot sizes of 3 assemblies. Battery will be assembled in our facility with the base and can held in place with Kapton tape. The entire assembly placed in a heat sealed pouch filled with argon gas and will be shipped to the supplier for welding. The pouch must be placed in an argon atmosphere before removing the components from the pouch for welding to prevent moisture from entering the battery case.