How about one of these.
How about one of these.
It's also available free (well, most of it is anyway) from Google Books
They're probably concerned about sparks flying, catching the rest of the state on fire.
You need to get the whole tire to about the same heat to get the stretch you need. How about using a DC welder, as they do to thaw pipes? That oughta work. They used to use a pine stick to test for the right temp. When the pine stick smokes and feels like it is "slippery" when pushed along the tire when it is touched to the tire, it is hot enough. I think that's about 700° F or so. You will need at least 4 supports under the wheel for the tire to stop at. More is better. Be ready with at least one helper. And have
4 or 5 pails of water sitting right by your setup to cook the assembly so it doesn't scortch to much. The amount of undersize that you will need will depend on how round the tire is and how round the wheel is. Also depends upon how tightly the wheel parts fit. If you start out with a tire about 1/8" undersize and it doesn't shrink up tight, you can shorten it and try again.I have only assisted in one session doing this to 4 wheels for a circus Hippopotamus wagon, but that's what I remember.
Pete Stanaitis
--------------------------------------------------
J. Clarke wrote:
Is this a permanent ordinance or one where there is a no burn edict leveled due to dry conditions that will be lifted after a rain?
Wes
How hot does it have to be?
The coefficient of thermal expansion for steel is 0.00000645in/in/deg F.
75 inches x 0.00000645 = 0.00048375 PER DEGREE INCREASE.So, how much fit do you need?
If you heat it up, and then slide it onto the wooden wheel. Won't that char the wheel some?
Six guys with six torches? When I was more actively doing HVAC. The boss and I would chit chat while we used two torches and two rolls of solder to assemble 1 1/4 copper pipe for boiler heat systems.
cavelamb fired this volley in news:B4SdnbFTn8xfWcnRnZ2dnUVZ snipped-for-privacy@earthlink.com:
Well, it ain't much, really. If you heated it up 500F, you'd get a 1/4" (roughly) circumferential expansion, which would be 1/4 over pi inches in diameter, or roughly a bit more than 1/16" diametral expansion.
That's enough, I'd say, to get it over a well-sized wheel. If not - if you wanted to pull the wheel together tighter than you built it - heat it up 1000F for an 1/8" increase.
On a wooden wheel, what you really need to do is make sure it will shrink down further than the amount it burns away the wood before it's below
450F. That's more dependent upon the skill of the wheelwright in mounting and chilling the tire than it is upon the actual temperature to which it's heated.LLoyd
"J. Clarke" wrote in news: snipped-for-privacy@news6.newsguy.com:
You've got 27" to work with if you put it in diagonally. There's a third dimension to be concerned about, but it's faster to try it than to work on all the calculations.
It doesn't matter if your oven tops out before the wheel has expanded enough, though. (But you knew this.)
Puckdropper
"Stormin Mormon" fired this volley in news:eI35o.33567$ snipped-for-privacy@newsfe04.iad:
It does, indeed. The "art" is in having it char away less wood than the amount it will shrink after cooling. There are ways.
LLoyd
In the time it has taken to discuss this, I would have dug a shallow hole, filled it with charcoal and done it. This is a classic case of overcomplicating things.
Not an option. If it was I would already have done it.
I'm with you on the ring. Should be real if possible.
How about a ring of charcoal brickets like used for the Bar-B-Que fires. Maybe a small hill in the center of the main ring circle.
lay out the ring on the ground - make a row inside and outside - then crunch them together, run a line of fire starter if you don't use auto-start ones.
So no real fire, just some bricks - and you can hose them down after wards.
Mart> Working on a decorative wagon wheel in wood, but I'd really like to put a metal
How do you figure? If I tilt it up front to back then I've only got the
21 width. If I tilt it side to side then I've only got the 17 depth.
Looking at this further, I may need a bigger tank than I'd want to handle to get this whole thing to red heat with oxyacetylene. Mongo weed burner is looking like the right tool.
On Sat, 31 Jul 2010 18:18:03 -0400, Usual suspect wrote the following:
-- To see what is right, and not to do it, is want of courage or of principle. -- Confucius
On Sat, 31 Jul 2010 12:11:32 -0600, Bruce wrote the following:
Have the womenfolk stand by with grilles and steaks once you move that damned tire out of the way of their cookout. ;)
Hmm, I don't think that'd do it.
-- To see what is right, and not to do it, is want of courage or of principle. -- Confucius
On Sat, 31 Jul 2010 13:09:02 -0700, "Artemus" wrote the following:
Yeah, make sure you quench quickly so it gets -brittle-, Arty.
The majority of the smoke is from when the tire cools onto the wheel and the wood burns a bit, but it's air cooled, not water.
-- To see what is right, and not to do it, is want of courage or of principle. -- Confucius
I don't understand something about this no-fire regulation. Where exactly is it that you can't have a BBQ? Seems outlandish.
RHave something to add? Share your thoughts — no account required.