Finishing an angled splice flush on a steel channel stair stringer

Nov 15, 2026 Last reply: 22 hours ago 3 Replies
Jump to replies (3)

Getting an angled splice on a steel C-channel to read as one continuous surface has to be the hardest part of this build, and West Weld attacks it methodically. The splice plate is beveled with a Fein angle grinder, held in alignment by locking C-clamps, then rolled inside on roller stands and welded with a Fronius TransSteel 4000 Pulse. The maker calls the result just grinding, but it is really a long chain of finishing steps.



The details that stand out are the tool swaps along the way. Pferd discs and a flap disc on a DeWalt cordless grinder blend the seam flush, a narrow finger sander polishes the inside radius, and a Milwaukee bandfile refines the inner corner fillet. Pneumatic and random orbital sanding follow, then a final hand pass with an abrasive pad. A metal ruler checks flatness across the joint, and a large evaporative cooler keeps the shop cool through it all.



Not everything came out clean the first time. Recent dual-shield beads on a test plate showed wormhole porosity, and the flatness check found slight low spots and pinholes across the joint. Those were filled with weld tacks and reground until the surface came even. What stays open is the exact cause of that porosity, which is left unconfirmed. Even so, the finished joint sits flush with the surrounding steel, and that even, continuous surface across the beam is the payoff for all the patience.



Project by West Weld. Watch it on their YouTube channel:

formatting link


The narrow finger sander for the inside radius looks like the smart pick to me. A tight interior bend on a channel is exactly where a flat disc runs out of ideas, so a narrow belt made for that radius, paired with the bandfile on the corner fillet, seems a well-matched pair.

One question on the weld side: was the pulse setting on the Fronius used for the splice weld itself, or only for the tacks that filled the low spots before the regrind?

For the wormhole porosity, a concrete thing to test would be longer stick out with dual shield, around an inch and a quarter, since that has been reported to avoid worm tracks. A quick bead on scrap before the next splice could confirm it cheaply.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required