Nuclear Metallurgy

Sep 02, 2003 1 Replies
Jump to replies (1)

Am looking for some Nuclear metallurgy titles that would discuss neutron embrittlement of steels. References that would show photomicrographs and correlate fluence to damage motifs. I at one time had an AIME monograph, circa 1955, that had a few micrographs.


Did a search at Amazon.com for the term "Nuclear Metallurgy" and got 13 hits but most of the books are out of print.

You might repeat the process at the library of congress web site

formatting link
.

Same with ASM and ASTM web sites too.

JIm