A welding/brazing decision

Nov 24, 2026 0 Replies

The mechanic I had working on the valves on my 1939 Harley flathead has screwed up - royally . The bottom end of the valve guide bosses on my rear cylinder have been damaged . Exhaust has a chunk broken out - I have the chunk - and the intake has cracks . This has caused the holes to bell at the bottom , which added to the taper at the top of the guides let the guides sit cocked in the holes , and this resulted in the valve seat being ground off center . So not only do I have to repair the guide boss , it looks like I'm going to have to install seats . Probably will do seats in the front too . I'm trying to decide whether to repair the guide bosses with Invar 42 or braze with phosphor bronze . I haven't yet begun to research seats , but if I can't find the guides I need I'll machine some from Ampco 45 .