It probably wasn't me that sent you the manual as Clausing only charges $10 for it and I feel that all but the most destitute owners should be willing to come with that much cash for a manual.
I may have sent you copies of the test report from my mill, though, or maybe scans from an old brochure showing the few accessories they sold for these mills. If you've lost those, or just want them, email me for a copy.
Mike
Didn't find your answer? Ask the community — no account required.
I posted this question before into a hurricane (as it were) of posts about the...
T
Terry Keeley
Thanks, I'll give him a try. I'm finding quite a variation in price for essentially the same bearings. The SKF bearings were quoted at $265 by Motion in Buffalo (or C$293 from Canadian Bearings here in Toronto) but the Bardens are around $320 or an incredible C$512 here. Must be using our old exchange rate of 60%!
T
Terry Keeley
T
Terry Keeley
I'm actually finding that a 15degree contact angle might be better for a milling machine as it can take higher radial loads with less deflection, 25 degree and up are better for axial loads.
T
Terry Keeley
Thanks for the kind words, I've have two buddies that have this mill and know what it's capable of. When shopping I looked hard at the "china mills", including the RF45 but just couldn't do it, even though I would have paid about the same as for this 1963 Clausing. It's going to be pretty as well as functional soon.
I've got a new Leeson 1/2 HP to go on it, woulda used a 3/4 HP but this one came cheap, not sure what you mean by a RIGID base but it has the standard mounting frame.
Thanks for the offers on the parts lists but I ordered a manual and parts lists as soon as I got the machine. I'm replacing all the bearings, the gears for the knee and the "y" nut, plus a few other odds and ends. The dealer I bought it from (Dick Treimstra in Detroit) even supplied an original inspection report from another machine (might be Mike's) so I can check mine when I'm done.
A
Abrasha
Check out this page:
formatting link
Go to page 7 of 16. The photo is of a resilient base motor. AS you can see, the base is a cradle that holds the motor around the shaft. On both ends the motor is mounted in a thick rubber rings, which allows for a certain amount of movement.
This is a rigid base motor:
formatting link
The base is welded to the motor.
Or look here
formatting link
under: "Type of mounts"
Rigid base Is bolted, welded or cast on main frame and allows motor to be rigidly mounted on equipment.
Resilient base Has isolation or resilient rings between motor mounting hubs and base to absorb vibration and noise. A conductor is imbedded in the ring to complete the circuit for grounding purposes.
Abrasha
formatting link
P
pentagrid
T
Terry Keeley
Oh, now see, don't think I've ever seen a resilient base motor, mines definately a rigid base with the NEMA 56 frame. Thanks for the help!
T
Terry Keeley
That's exactly the case with the 8520 spindle, they use a single bearing near the top with a duplex pair at the bottom. Somewhere in my reading I recall that back to back mounting is a more rigid set-up.
N
Ned Simmons
G
Gunner Asch
M
Mark Rand
N
Ned Simmons
N
Ned Simmons
Can you explain that notation, please? Your post makes sense to me if is face to face and >< is back to back, as illustrated here...
formatting link
I don't recall ever seeing that notation and it seems backwards from the way bearings are usually drawn.
Ned Simmons
T
Terry Keeley
The inner races are clamped together with a locknut, is that the proper condition for back to back mounting?
J
jim rozen
For angular contact pairs, whether back to back or face to face, the outer races and inner races *must* be clamped together.
The inners via the spindle nut and whatever spacers stack happens to be there, the outers typically by clamping them in a bored recess with a clamp ring.
In both ff and bb mounting, you will see that locknut. You cannot determine a priori one vs the other because of its presence.
Jim
J
John
V
Vince Iorio
Like most of you all, I save everything ...
Here are the bearing numbers I received when buying the bearings from Clausing several years ago (I still have the empty boxes).
Two Fafnir 7205W SU bearings. The boxes were taped together and I believe they were the lower spindle bearing.
Two Fafnir 9105KDD bearings. I believe these were for the front pulley.
One Fafnir 204KDD bearing. I believe this was the upper spindle bearing.
One CR Services 13548 Oil Seal. This is for the bottom of the spindle.
As the directions posted by Mike says, the bearings are Back-to-Back. As I think back to when I was doing this, I recall putting them in backwards first. The advantage of the back to back configuration is when pressing the bearings out you are NOT reverse loading them. In the face to face configuration you are loading one of the bearings in the wrong direction when pressing them out. This might be a problem if the press is high, and you want to reuse the bearings.
IAW my Fafnir catalog, the "SU" means the bearings are packaged singly, and can be used DB, DF or DT (Tandem). "DU" in place of "SU" means you will get 2 "SU" bearings in one package. Might be a price brake that way.
There is a difference between the "W" and the "WN" that Mike quoted. I don't see a 7205WN in the catalog, just a 7205W. The "W" has a 20 deg contact angle, and the WN would have a 40 deg. It is only the smaller sizes that are "W", so I am guessing that they are to small to make with a 40 deg angle.
FWIW, after I got the bearings from Clausing, I priced them out from a bearing house and they were about a 1/3 cheaper.
Hope this helps.
Vince
Mike Henry wrote:
G
Gunner Asch
As you will notice..angular contact bearings are essentally cone shaped in their bearing contacts. One side of the bearing has a wide gap around the race, the other side has a much narrower gap.
They are designed to basicly be pushed from the wide..or thrust side, so the bearings are forced deeper in to the cone.
Hence the >< being two cones facing each other with the thrust towards each other being applied by the shaft and lock nut that pulls them deeper into their respective cones.
If you reverse the arraingment in a fashion..the shaft and nut Pulls the inner races away from the cone. Even with a preload cylinder between them..thrust makes the bearing move towards the wide end of the cone..away from full contact. \-----\
----- thrust------> >
/___/
Even if the two cones >< are seperated by a short distance..they are pulled deeper in the races by the lock nut.
I dont know the nomenclature for front and back..but only know them as thrust side and the other side and the thrust side (often plainly marked as such) need to be on the outside of the bearing stack, and pulled together, then the entire bearing group held tightly in the housing. Ball screw thrust bearing (double bearing) packs have a removable "cover" that is held in place by bolts/screws that keep the outer races held rigidly in place.often with a very thin spacer that contacts only the facing faces of the outer race.
Hope that helped, not confused..and that diagram in your link..is >< as you indicated
Gunner
"Pax Americana is a philosophy. Hardly an empire. Making sure other people play nice and dont kill each other (and us) off in job lots is hardly empire building, particularly when you give them self determination under "play nice" rules.
Think of it as having your older brother knock the s*it out of you for torturing the cat." Gunner
N
Ned Simmons
That clears it up - I've just never seen the / >< notation to indicate mounting arrangement. It seems the way to think about it is that < is a representation of the shape of the races, whereas the notation I'm used to, as shown on that KOYO page, represents the contact angle between the ball and races.
Ned Simmons
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?
Ask the community — no account required
Report Content
You are reporting this content to the moderators. They will look at it
ASAP.