There is, or used to be a large jewelers supply in Albuquerque called Rio Grande Jewelers Supply. They carried all kinds of refractory material for casting & silver soldering. I specifically remember white soldering blocks that were made from Alumina if I recall correctly. Take…

Read the full reply

I'm looking for Fiberfrax (or similar) boards and insulating firebricks (the soft, lightweight kind) for building a temporary, reconfigurable forge. I've tried a couple of local brick suppliers and have been going through some Google hits with no luck so far. Does anyone know of a supplier for these in Albuquerque, or possibly a reliable online supplier that will sell small quantities?



Thanks. Bert


There is, or used to be a large jewelers supply in Albuquerque called Rio Grande Jewelers Supply. They carried all kinds of refractory material for casting & silver soldering. I specifically remember white soldering blocks that were made from Alumina if I recall correctly. Take a walk through the Yellow Pages. Bugs

Must not be a lot of hot furnaces in NM?

Go here, look around, but the nearest for you is either Texas or Utah, bummer...

formatting link

============================================== Put some color in your cheeks...garden naked! "The original frugal ponder" ~~~~ } ~~~~~~ } ~~~~~~~ }

formatting link
fiberfrax in small qty.

Larry is great to deal with, I've bought several times from him:

formatting link
Jay has a good reputation, I haven't bought from him:
formatting link
But in Albuquerque it should be pretty easy to find a local supplier. Watch the price, it can vary a lot. I used to buy from Renler in Englewood, Colorado, they were pretty reasonable.
formatting link
Steve

Have you tried

formatting link
?

Don't specifically recall seeing firebrick, but they had kiln cement when I shopped there 7 years ago.

you can get frax blanket or boards in 1" or 2" thickness on ebay pretty cheaply.

regards, charlie

formatting link

The soft, insulating firebricks are good, but they are rather fragile when at temperature. The heavy-duty ones take longer to come up to heat, but are much more sturdy. You might want to use heavy-duty bricks in the floor of a forge, or any place the bricks might get knocked over...

I'm using stacked bricks for the mouth of my forge. It's easy to hook the end of a piece and pull over the bricks when taking something out of the forge. I've done it a couple of times...

I have a bunch of Fiberfrax-----did you get my reply of 10 minutes ago?? it didn't show up in my "sent" file---Jerry

dwarf.nntpserver.com!statler.nntpserver.com!newsfeed-west.nntpserver.com!f

It appears that you tried to post a binary. Don't do that.

dwarf.nntpserver.com!statler.nntpserver.com!newsfeed-west.nntpserver.com!f

Sorry 'bout dat--I thot I was replying to the original poster ONLY--Jerry

>

I'm currently looking for board, not blanket, but I'll keep you in mind if I ever get around to building a more permanent forge.

Bert

jerry wass wrote:

Their website does show firebrick, but no Fiberfrax board. Their bricks are a little pricier than other online sources, but since there would be no shipping they may end up close to the same. Thanks for the info.

Bert

Thanks to all who responded. In case anyone is interested, here's what I found on the suggested websites:

formatting link
- couldn't navigate beyond the home page (could be a browser issue)

formatting link
- no bricks or refractories

formatting link
- Fiberfrax blanket but no board; no bricks

formatting link
- Fiberfrax board and blanket, no bricks

formatting link
- ceramic fiber board and blanket (brand not specified), no bricks

formatting link
- no bricks or refractories

formatting link
- bricks, Kaowool board and blanket

formatting link
- Insboard, Inswool, bricks

how much do you need? a bunch of us recently got together and purchased a palette of 2" vermiculite boards from europe, but that's a lot of board. there isn't any left, but i can get you a contact for the person who set it up.

Look also for "boiler liners".

LLoyd

I've bought from budgetcastingsupply - still have some at hand and good product.

Perhaps the issue on the

formatting link
- it uses java to point to the various pages. Must have java enabled.

Have you checked the local fireplace, ceramics, etc supply house in town ? or near by ?