I am the defacto primary gunsmith for the MIT collegiate pistol team. They have a large number of Czech CO2 pistols that were made about 20 or more years ago. They shoot very accurately, and are generally pretty reliable. The primary firing seal is dying on a few of them, and the replacements we have don't fit due to a design change at some point.



formatting link
The seal is a short hard white plastic tube, press fit into a hole in the pistol frame. The actual firing seal is formed with a conical pin that presses into the hole through the center of the plastic seal. On the theory that the most likely seal material is Nylon 6/6, I bought some rod stock, and I'm going to try making new seals from scratch.



The recommended approach for removing the old seals it to run a brass wood screw into the seal & then pull it out. The pulling part takes quite a bit of force, and the process means the seal can't be re-used once removed. However, the one I extracted is sufficiently intact to take some measurements from. Give or take a few tenths, the seal measures 0.3157" OD. The bore in the pistol measures 0.3138" ID.



I've done some reading on both Nylon & press fitting plastics, and there are several issues that complicate matters:


1) Nylon is hygroscopic, and will swell depending on the moisture content. That means if I machine one now when it is humid, it will shrink in the winter. On the otherhand, machining it will heat it a bit & dry it out slightly.


2) Nylon has a pretty high thermal coefficient of expansion. That means I probably need to let it cool off to measure it when I'm machining it. They recommend chilling the part to shrink it for the press fitting, but with high humidity, if I get it at all cool, it will be covered with moisture (if not frost). I'd have to drop the temperature ~ 60 degrees F to shrink the part by 1 mil, which definitely gets it into the frost category.


3) If I make it sufficiently oversized to make sure that moisture & thermal variations don't allow it to shrink enough to be a problem, it can creep over time & loosen up. I suspect that may be why some of them are failing after all this time, possibly shrinking enough to allow CO2 to sneak past them. There's a good web site that talks about this here:

formatting link
This also means that the measured size of the seal I removed is probably smaller than it was originally cut. As extracted, they had about a 2 mil interference fit, which would seem to be plenty. I need to double check the calculations, but that should result in over 1500 psi of expansive force between the seal & the bore of the hole. It's also enough to produce significant creep over time:



formatting link



1% is over 3 mils, although as it creeps, the forces will drop, and presumably it will reach something like steady state when the force drops enough.


4) Annealing: Lots of folks recommend annealing Nylon before trying to machine it. From some DuPont literature, 3/8" rod stock should only require an hour at a couple hundred F. They recommend not doing it in air, and suggest heating it in wax or oil, and then cooling it slowly & evenly to avoid surface stresses. I'm thinking heating it in cooking oil with a thermometer, and then letting the whole mess cool slowly.



There are other plastics that have lower moisture issues than Nylon 6/6, but I think the TCE & creep is going to be similar for a lot of them.



I seem to have opened a serious can of worms here. I'm thinking about just going for it, cutting one 2.5 mils oversized without annealing. If anyone has any real experience to help sort through the chaos, I'm all ears.



Thanks!



Doug White


Try pulling the seal with a brass screw fitted in the head of a small slide hammer. Available at Harbor Freight for less than $15.

It could be Acetal.

I recently made a replacement lighter plug tip retainer from a Nylon spacer and some larger Acetal rod. Both machined nicely to intended size with a good finish, including on the single-pointed threads.

Before someone asks why bother, it's on an Auto-Air laptop charger and the Air jack is in the back end of the Auto plug.

jsw

Page 19 of this guide has some guidelines for press fitting for various filled nylons and other plastics as well as the effets of water absorption. They seem to indicate it is mainly an issue in wet environments.

formatting link
If wear is an issue, you might want to look into one of the filled nylons.

Have you contacted Beeman? They used to sell Czech air guns and may still do. They have a large repair dept which may even have the part you need.

formatting link

I would het the nylon to be sure the moisture is out of it, then machine it over sized enough to counter the effects of the CO2 on the seal. If you're really worried you could contact Crosman and talk to them, They use plastic valve seats in most of their items and might be able to tell you what you need to know. 800-724-7486

azjohn wrote in news:jt7pfo$4jo$ snipped-for-privacy@wieslauf.sub.de:

If the re-sealing is a success, I will get more serious about tooling up to fix more in the future. I had envisioned a threaded tool where you screw the brass wood screw into the seal, and then run a nut down a threaded piece to extract the old seal.

Doug White

"Artemus" wrote in news:jt7vcv$6k1$ snipped-for-privacy@dont-email.me:

I've tried a number of places, and the few that have seals don't have the size I need. So far we've identified at least 3 design variations with different sized seals.

I checked Beeman's site. As far as I know, they never sold the Tau-7's, and they don't list them as a make/model that they service.

Doug White

"Jim Wilkins" wrote in news:jt7qa0$8ll$1@dont- email.me:

I thought about that. I went with nylon because it is more impact resistant, and the metal firing valve whacks into it with every shot. I also figured it's a more likely material for a non-high-end commercial product. Now that I have all the measurements I need off the original, I can try to burn a sliver & see if it burns & smells like nylon or not. There's a useful chart here:

formatting link
but I also have known samples of nylon 6/6 & acetal to compare with.

Doug White

"Steve W." wrote in news:jt7vqo$8bm$ snipped-for-privacy@dont-email.me:

Neither one lists any Czech air pistols, although JG seems to cover enough bases that I'll send the an email, just in case.

Thanks!

Doug White

Gunner Asch wrote in news: snipped-for-privacy@4ax.com:

Do you mean HDPE? I thought about UHMW PE. All three materials are much softer than the original seal. I'm concerned with cold flow. The valve seat is under considerable pressure, and a soft material could mush down & cause problems. They can also be even nastier to machine than nylon. I'm fighting with some UHMW on another project right now.

Doug White

Yes, but the worst that can happen if you call them is they'll say "no" and hang up. At best you'll get the parts you need, so unless you're looking forward to making these critters, it doesn't hurt.

You might want to do a flame test.

formatting link

I used to work in a semiconductor plant that used a lot of Nupro Valves, they all had Kel-F stem tips, very hard plastic but with chemical properties of Teflon. Most likely very expensive.

formatting link

No idea what it machines like.

ebay item Item number: 230806546854 1/2" rod 12" long

or search ebay for kel-f or pctfe

this might be the high tech replacement for whatever was there.

Remove 333 to reply

My gut reaction is to scare up a native speaker of Czech and call the manufacturer.

The manufacturer will have someone who understands English, even if they can't quite speak it over the phone. So send them a letter first. When writing the letter, stick to short simple sentences and no slang.

Joe Gwinn

That's another option, but for someone who is on staff at MIT it seems to me that calling admissions and asking if there's a Czech enrolled would be a fairly simple first step.

Ahh. Not a widely-available option, but it ought to work.

Joe Gwinn

Maybe a small wood stud? Wood screw on one end an machine threads on the other.