Strength of aircraft grade versus 6061 aluminum?

Oct 07, 2008 41 Replies

Planning to use a short piece (2 or 3 inches) of 5/8" outer diameter aluminum tubing. The wall thickness will be 1/16" to 1/8".



Pressing down on the center of the tube will be a maximum momentary pressure of very roughly 300 pounds (a wild guess).



Is there any difference between 6061 aluminum and aircraft grade aluminum for that purpose?



General ideas about the differences between the two would also be appreciated.



Thanks.


FWIW: With the aluminum tube end inner surface roughened, if I can get the inner diameter correct so that the aluminum tube end can be glued snugly around the motor gear, that should be straight and hold very well. The aluminum tube might also provide good heat sinking when spinning fast.


formatting link
Both yield and ultimate tensile for 7075-T6 are at least 80% higher than 6061-T6.

Is "aircraft grade" something like "industrial strength" or "heavy duty"?

Surgical Stainless Steel?

What you really want is "audiophile - quality Vulcanian billet".

--Winston

The three word term "aircraft grade aluminum" in quotes produces almost one million results on the Yahoo search engine. The term is commonly used (and defined) at McMaster, a huge metal parts supply merchant on the web at

formatting link
and physically located in the United States.

Not exactly. Certain grades of aluminum were developed from need of the aircraft industry. They are, in general, very much stronger when heat treated (or aged) than other grades of aluminum. 7075 is likely the strongest (it rivals mild steel in tensile strength when aged to a T6, or T651 condition, with 2024-T351 being quite good as well.

Harold

Alloys are not grades. The term "aircraft grade" is simply inept puffery in this context.

7075T? also considerably less ductal that 6061-T6...

If that matters in this application.

"Aircraft Grade" sounds better than "beercan grade".

The poles for my extremely light Stephenson tent are 7001(?) aluminum tube, 5/8" OD,

0.015" wall. (Jack was once an aerospace engineer.) I picked the tent up at his house and he showed me how strong the poles are by placing a 16" piece on blocks and having me stand in the middle, barefoot. OTOH the alloy cracks easily and is 'notch sensitive'. I split the end of one of the sections by tying it down a little too tightly on my motorcycle with bungee cords. The tent still stands with one taped break but it loses some wind resistance. While I was there he got a call from someone camped on top of Mt Washington whose tent was surviving a 125 MPH wind.

As I understand it, 6061 is the strongest alloy that doesn't have corrosion, brittleness and joining issues requiring extra engineering analysis.

Jim Wilkins

I should have mentioned that they are very open-minded 'naturists' and the web site may not be entirely suitable for children.

It's thrown around pretty loosely these days, but the term originally referred to the aluminum-copper alloys developed in Germany around WWI, which were given the name Duralumin. They were similar to today's 2024. Then other precipitation-hardening grades were developed, and the term today usually refers to 2024, 7075, and maybe a couple of other grades in the

2000- and 7000 Series.

But it's become a marketing term, like "billet," so you can't count on it referring to a particular grade anymore.

-- Ed Huntress

On Mon, 06 Oct 2008 23:58:07 -0700, the infamous Winston scrawled the following:

Right. One can't beat the oxygen-free, audiophile-quality, Vulcanian billets of aloonimum, can one?

Besides price, yes that matters. I'm probably going to struggle just to get the fit right without grinding the motor gear, so being ductile is potentially important. I'm also looking at some sort of nylon/whatever thin tubular spacer if necessary to decrease the inner diameter of the aluminum tube.

But I'm curious about aircraft grade aluminum too. So far I picked up at least two different numbers (2024, 7075) designating aircraft grade aluminum, and the idea that metal can be hardened with aging (didn't know that one).

Thanks to the replies.

Look up precipitation hardening of aluminum. That's a more precise name for "age hardening." Some grades harden that way. Others don't.

-- Ed Huntress

  1. As you've found out, there are different "aircraft grade" aluminum alloys out there. Think about specific alloys, not "aircraft grade" vs. "landfill grade" (although I haven't seen any Al marketed as "landfill grade". I wonder why?).
  2. Why not 5/8" rod, with an appropriate sized hole in one or both ends?
  3. My intui-meter tells me that 300lb on a 1/8 wall 5/8" diameter
6061-T6 tube ought to be OK. Do you have reason to suspect otherwise? 3a. It makes a big difference how and how often this load will be applied -- with a sharp edge? Squishing the tube? Trying to rip the tube off of the shaft it's mounted to? What?

Ed My son had a project where he built jet engine hangers for a new, more powerful C7 military transport jet engine. The billets for this project were

4" thick by 48" by 144". "The Kid" only knew it was a special military grade AL alloy. He brought home a pile of scrap from this job. Any way to guess what this stuff is and its properties? I've got a few hundred lbs.

Karl

Ed,

The story of the development of precipitation hardening aluminum alloys is quite interesting.

Recalling from memory... One investigator was showing two visually identical strips of copper-bearing aluminum alloys to a colleague and asked him to bend them by hand. Although identical in size and alloy, one could be bent and one could not. The difference was the precipitation hardening.

The discussion turned to the % composition. Much of the early work was based on experiences with copper alloys such as brass and bronze, where the alloying constituent may be from say 5% to 40%. And aluminum bronze is an alloy of approx. 10% Al and 90% Cu, forming an exceedingly tough and abrasion metal.

The investigator stated that the copper content was less than 1% and closer between .25% and .5%. The colleague asked "why so little" and the reply: "In steel alloys you only have carbon content at typically less than 1% also. When I first read this tale in a book entitled "Metall" 40 or 50 years ago I was fascinated.

Wolfgang

In a word or two. Forget the "buzz words" and learn what the aloy numbers mean and USE them. ...lew...

In my signature, you see "rollerblades". Strictly speaking, that should be "in-line skates", but most people couldn't care less and "rollerblades" makes perfect sense to the vast majority of readers.

This skate looks like it would way upset the proper balance of the toes and ball of the foot over the leading edge of the skate?

The problem is, there are several different "aircraft grade" aluminums

- of which 6061 T6 is one. All Zenith aircraft are built almost exclusively of 6061 T6

6061 T6 is les likely to crack when bending than a 7000 series in T6. T6 is a hardness spec (solution heat treated and aged IIRC) and is harder than T3 or T0 (normalized) ** Posted from