You know I started my journey into mold making and machining in general right here in this group. While I am far from a master at anything sometimes people just know how to piss me off.



When I started learning to machine fishing lure molds from Aluminum I fought flood coolant with a passion for clean dry chips. I may not have tried everything, but I tried a lot, and kicking and screaming I finally got dragged into the deep end of the coolant tank.



Air doesn't even work 90% (works pretty good on steel).



Vacuum works less than air.



Mist doesn't work, and actually can trap chips instead of blowing them clear in deep slots and deep pockets.



MLQ doesn't work 100% and can have some of the same issues as mist. Its basically mist.



I never tried alcohol mist, but I can see potential for some kinds of work other than the hazardous environment.



Flood oil actually worked pretty good, but its burns up and it gets expensive.



Coatings are pretty much a waste of time. Some coatings are worse than a waste of time. I tried all the wrong coatings and many of the "right ones like ZrN and PVD Diamond.



Plain bright polished carbide end mills and water soluble flood coolant just work. I spent years getting that beaten into my thick skull by fighting against it.



Today some flyby expert went on one of my videos and said I should use some "name brand" of end mills and ditch the coolant for air. Instead of asking if they really had a 1/16 long reach ball nose end mill that would run as fast and as cleanly deep slotting to a depth of 0.412 inches, I just deleted his comment.



The point of my video was for people to go, "Oh cool. A mold." not get information or in my opinion bad information, about how to make one.



Thanks for all your help guys. Those of you still with us, and those of you who aren't.


Just a couple of daze ago I finished a *little work on a friend's ATV . I don't charge labor for friends and neighbors , but if a bottle of Wild Turkey shows up ... So have a shot !

  • front CV axles , choke/enricher cable , and fuel pump

I suppose it depends on what machines you have and whether they're enclosed. I've mainly used coolant on manual machines and it can get messy but then I've seen enclosed machining centres designed for flood coolant where when it starts up you can't see what's happening due to the coolant getting thrown all over the windows.

Helped a friend working on one of his friends' cars today - a 2012 Civic with almost 300000 on the clock - and original rear brakes. I had to use the death-wheel to cut the drum in half to get it off. No loss as it was over 120 thou oversize. Then we had to change the starter. Any of you brave souls attempted that on a civic 1.8????? Between the brakes and stater - NOT including cutti g the drums off yesterday, the two of us were at it for 5 1/2 hours - and neither one of us are Noobs (except on 2012 Civics) Don't charge friends - or even GOOD friends of GOOD friends. Dealer labour estimate was $850 -__-

On Thursday I have a "simpler "job - just replacing a left rear axle bearing assembly on a rusty 2010 Sienna - for another friend. It's a half hour job that I am certain will take at least 3 - - - - I've been wrong before, and hope this is another of those rare times!!!! Changing the serpentine belt on that critter 2 weeks ago took me 2 hours - - - - - - (over 220000 MILES on the original belt - - - - -)

Today I worked on my own ATV , a 2007 Arctic Cat 650 . It was gifted to me because the previous owner didn't want to do all the repairs it needed ... I know now why he gave it away , I'm several hundred bucks into it for just the parts . The latest repair was to the starter system . The overrunning clutch on the flywheel was jammed , and the starter was spinning the whole time the motor was running - at about 10X the crankshaft speed . Wore the splines right off of 2 starters ... the hardest part of the whole job was pulling the flywheel . Keyed taper , I finally got it off by heating the hub with a magnetic induction heater and dribbling liquid propane on the shaft .

Helped a friend working on one of his friends' cars today - a 2012 Civic with almost 300000 on the clock - and original rear brakes. I had to use the death-wheel to cut the drum in half to get it off. No loss as it was over 120 thou oversize. Then we had to change the starter. Any of you brave souls attempted that on a civic 1.8????? Between the brakes and stater - NOT including cutti g the drums off yesterday, the two of us were at it for 5 1/2 hours - and neither one of us are Noobs (except on 2012 Civics) Don't charge friends - or even GOOD friends of GOOD friends. Dealer labour estimate was $850 -__-

On Thursday I have a "simpler "job - just replacing a left rear axle bearing assembly on a rusty 2010 Sienna - for another friend. It's a half hour job that I am certain will take at least 3 - - - - I've been wrong before, and hope this is another of those rare times!!!! Changing the serpentine belt on that critter 2 weeks ago took me 2 hours - - - - - - (over 220000 MILES on the original belt - - - - -)

------------------------------ The nation that gave us Origami and Transformers uses their skill to pack components tightly with only one secret way to disentangle them. Removing the alternator or starter from my 91 Ford takes maybe 5 minutes, on the 2000 CRV changing the alternator was an all day job, some of it removing other things to clear an exit channel. The pivot bolt was hopelessly corroded steel-to-aluminum and the mounting bracket bolts had fine threads with over an inch of engagement and only enough clearance to turn a 12 point wrench one notch at a time.

I'm getting too old and sore for the under dash contortion that both have recently needed. At least the Ford's carpet is clean after being removed, hung up and hosed.

A neighbor has less trouble finding parts to restore a 60's Chevy than I do for my much newer but not classic vehicles. The other neighbor has a friend who visits in a 1931 Ford restored to showroom condition with original parts. I had a relative in Alabama who still drove his 1935 Chevy pickup.

NH has officially discontinued yearly car inspection but some shops will still do a low cost advisory inspection for those who care.