Tinning Copper saucepans - again!

Feb 21, 2006 4 Replies
Jump to replies (4)

I've read the previous threads on this subject and need some help making them come together. Bought my pure tin, tallow, and Bakers No5, Scoured my pan with de-greaser and dipped in caustic soda to be sure of getting rid of the grease, Wire wooled the surface Applied the Bakers No 5 flux by poring it in the bottom and wiping around the sides with an old rag. First tried to heat the pan with a blow torch - but couldn't get the all-over heat. So put the pan on the stove. When hot enough put a tin stick in the pan and it melted easily on the bottom. However the molten tin went into pools and wouldn't adhere to areas of the pan bottom or the sides - it just flowed over these areas Any suggestions on what to try next would be greatly appreciated Are there any web-sites with step by step pictures ? DO I need more heat



thanks



Denis



Despite the fact that you are sure that you've cleaned everything perfectly, evidence (tin flowing over areas of the pan) would suggest that you have not, or that you have allowed them to become oxidised again after cleaning. More heat is more often a problem than a solution in soldering (of which tinning is a specialised branch) - in fact, overheating areas is one way to make them not take tin.

Putting the pan on the stove to heat it could cause cleaned surfaces to become oxidized. Can you suspend it above the burner to heat it up?

Ecnerwal wrote:

you are working too hard - just put in a spoonfull or two of plumbers flux (the acid stuff that come s in tubs), heat the pan on the stove and scrub with steel wool (while it's hot enough to melt the tinning) when everything is covered, wipe with a paper towel to spread tin evenly and let cool, then wash off hte acid flux

I've d>I've read the previous threads on this subject and need some help

Bill

formatting link

to contact me, do not reply to this message, instead correct this address and use it

will iam_ b_ No ble at msn daught com

*** Free account sponsored by SecureIX.com *** *** Encrypt your Internet usage with a free VPN account from
formatting link
***

Was your steel wool de-oiled?