Where to apply the heat

Oct 12, 2010 23 Replies

Yeh, I saw that he said he didn't want to overhaul now. But, is it one engine or two? 16hp--- sounds like a 2 cylinder?

Pete Stanaitis

-------------------

RBnDFW wrote:

I've used the ATF and acetone mixture for removing a Marlin 39 barrel from a 60 year-old gun. Soaked it for a week, came loose with the first whack on the receiver wrench. Before that, it was stuck solid.

60 years of .22 residue will do that.

Stan

Okay, here we go again: Saw off the pipes as needed. Thread the ends and attach fittings.

---or---

Saw off the pipes as needed. Weld or braze new tubing onto the ends.

I say these things because I have had such poor success getting steel out of aluminum, even in much smaller sizes.

See:

formatting link
Pete Stanaitis

------------------

snipped-for-privacy@aol.com wrote: