110 VAC arc welder success stories?
Jun 12, 2005
24 Replies
I checked my 110VAC welder. It uses isolation.
BTW With 35 amps 110VAC and fand cooling added it is now burning 1/8"
6011 with 100% duty at 100 Amps.BoyntonStu
Glenn,
Exactly! That is why I shared it on the net.
It is so obvious now that I have it working.
If you would like to see a few of my other 'wild' ideas, that were also blasted by naysayers prior to my doing them, write me off list.
BoyntonStu