what diameter wire to use to get 3/4" fillet in 1 pass?

May 31, 2013 1 Replies

First reply

Ernie Leimkuhler

My guess would be a 3/32" wire running on a 600 amp machine. In theory you could do it on a 400 amp machine with 1/16" wire if you went slow enough, but you would likely fry your stinger if it isn't water cooled. Most welds that big are either multi pass or sub-arc welded.

Read the full reply

What diameter wire to use to get 3/4" fillet in 1 pass on 1 1/2" thick steel plate?


My guess would be a 3/32" wire running on a 600 amp machine. In theory you could do it on a 400 amp machine with 1/16" wire if you went slow enough, but you would likely fry your stinger if it isn't water cooled.

Most welds that big are either multi pass or sub-arc welded.