⚗ Material Sciences

1792 Threads Posts
to

wear testing

can anybody provide me guidance in wear testing for analysis of wear mechanisms in steel??? will Pin on disc method work...
1 comments posted 20yrs
posted by billghutes1
1 comments posted 20yrs posted by billghutes1

polylactide

hi i am facing difficulty in synthasising PLA by ROP. i am getting very lettle amount of lactide from lactic acid
0 comments posted 20yrs
posted by vimalkumar.7
0 comments posted 20yrs posted by vimalkumar.7

Diamonds in the Spring of 2006?

Spring 2006 is about to be over, Uncle Al! Any news on your diamond synthesis experiments you would like to share...?!...
0 comments posted 20yrs
posted by k.a.cherian
0 comments posted 20yrs posted by k.a.cherian

thin al alloy

I am desperately searching for some Al alloy sheet of thickness 0.2-0.5mm. I cannot find any suppliers that do them this...
1 comments posted 20yrs
posted by eazap1
1 comments posted 20yrs posted by eazap1

C75 corrosion

Hi everybody, I need a suggestion, how is the resistance of C75 quenched steel (C 0,70=F70,80 % Mn 0,60=F70,80 % Si 0,1...
0 comments posted 20yrs
posted by circio0
0 comments posted 20yrs posted by circio0

Looking for grainless plastic sheet

I'm looking for thin (ideally .010 or even thinner) plastic sheeting that's semi opaque/translucent - sort of like "mil...
14 comments posted 20yrs
posted by muzician21
14 comments posted 20yrs posted by muzician21

the latin word for knowledge is science

So would a scientist be essentially a knowledgist per the meaning of the word science? Is there such a word as knowledg...
0 comments posted 20yrs
posted by scott
0 comments posted 20yrs posted by scott

Au nanoparticles

I am interested in characterizing Au nanoparticles dispersed on flat surface. When using diffraction technique, e.g. X-...
0 comments posted 20yrs
posted by murooka
0 comments posted 20yrs posted by murooka

Looking for "Thermal Comparator" info

I may need to measure the thermal conductivity of a thin film. From the searches I have done so far, it is clear that s...
1 comments posted 20yrs
posted by nospam
1 comments posted 20yrs posted by nospam

Quality control at the nanoscale.

This article discusses new research doubting nanotubes could provide sufficient strength for a space elevator: Nanotube...
0 comments posted 20yrs
posted by rgregoryclark
0 comments posted 20yrs posted by rgregoryclark

Carbon-Carbon For Solar Engines

Has anyone done anything with carbon carbon for closed cycle engines? With solar you can have 3000 degree inlet temperat...
0 comments posted 20yrs
posted by BretCahill
0 comments posted 20yrs posted by BretCahill

Stainless steel magnetic?

Hi all, I've an issue on stainless steel. I've got some product, that my supplier claims is stainless steel. However, a...
15 comments posted 20yrs
posted by wouter
15 comments posted 20yrs posted by wouter