How to avoid Ferrit??

hello,
im casting pig iron with high amount of phosphor ( about 3 percent) and i get 40- 50 percent Ferrit. by 1,5 percent phosphor i dont have such problem ( 8-10 percent ferrit)
does anybody have an idea what i can change the time from casting to unpacking is about 1 hour