T314:

formatting link
No time to look up more information right now referring to heat resistance. However, it has been used for years in brazing and heat treating furnaces including direct natural gas fired furnaces.

Koz

That was more than enough to answer my questions. Thanks.

314 appears to be very high in both nickel and chromium as compared to 316, which likely accounts for its heat resisting quality.