Drill Doctor 350X!

May 03, 2012 7 Replies

Maybe it was a waste, but it was only $50 and I enjoy doing things right.



Should the diamond grinding wheel or the bit being sharpened be wet with some liquid like silicon or WD-40?


I also made a channel to help cut my aluminum flat bar forks. Haven't used it yet, but it will help do it right.



formatting link


It is not diamond, it is CBN.

i

i run my Darex drill sharpener dry

I don't know if you can even use coolant with a Drill Doctor, but with a CBN wheel, don't use coolant with a rust inhibitor in it. The chemistry isn't compatible. (Something I learned by interviewing wheel manufacturers a decade ago.)

Ordinary soluble oils are recommended in production and toolroom applications.

Don't lube the drill doctor.

It is best not to practice to many times with expensive stuff :-)

Mart> Maybe it was a waste, but it was only $50 and I enjoy doing things > right.

That conical shape won't work very well, but they have another cut that will.

I've recovered a broken 3/4" drill I got for free. I first turned it like that and then cut the cross point. Another one, I corrected to that form and then hand ground the flats on it.

What is the other - cross point ? something like that.

Mart>

formatting link
>

They are the same 1/2 inch drill bit, with different lighting Number 2 is after another grinding.

formatting link

I might try sanding the cutting edge with a rotary tool. That would be my first use of a rotary tool sanding paper disk.