Explosive forming

Dec 30, 2003 28 Replies

formatting link
I'd start there. That's Mine Safety and Health Administration, the folks that certified my instructor.

Jon

I'm surprised a plaster form worked. I would have thought the plaster mold wouldn't hold up to the explosive force. Was is very thick? What kind of metal was he forming, and what was he using for the explosive?

Lane

That's a cute idea. What I would like to know is if the water moved it out of the way , all the gravel and rocks would be different. If what their after doesn't move then it must be drilled and blasted out anyhow. Or maybe they just wanted to get equipment past...

We were dredging for gold, which has an amazing afinity for burrowing into any sort of crack, hole, or banking up against any abrupt ledge. In addition, gold settles out where water speed drops. The pool in question was just below a fairly narrow solid rock 'valley' (for lack of better description). Bedrock here was composed of rock similar to slate, with vertical cracks perpendicular to the flow of the stream, great riffles for fine gold. It was just below a depression era mining camp, and was probably the best spot for hundreds of yards for dredging.

I only went back one more time after that boulder disappeared, and I don't know if the owner of the claim ever (literally) struck gold in that pool.

Jon

Sorry, I just knew I should have read your post again. I just recalled the word placer and thought that meant hard rock mining and crushing like with the steel balls that I have from old mines.

I've always wanted to find some gold , any at all. It sure must be really rare cause I've searched in a lot of prime locations. Kinda like my unsuccessful hunt for a meteorite.

Since my early teens, I'd wanted to find enough gold to make my wedding rings, come the day. Can't count the hours I spent digging, panning, crevicing. Came the day, and I had but one tiny nugget to contribute. Our rings prominently feature small nuggets, and the one I found graces my wife's ring.

Jon

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required