It's in a somewhat modified cargo aircraft- a new kind of commercial surveying system. The helium just keeps the innards very cold.
Best regards, Spehro Pefhany
It's in a somewhat modified cargo aircraft- a new kind of commercial surveying system. The helium just keeps the innards very cold.
Best regards, Spehro Pefhany
One possibility is to use a graphite based thread sealant, like:
The threads have to be reasonably good for that to work.