Currently I'm waiting to get the transformers. They're very heavy and I need my father to pick them up in his estate car or trailer. In the meantime I'm doing some work to renovate the motor. Last night I removed the pulley from the motor shaft. It's secured with a taper key and after
70-odd years it was stuck on there pretty tight. I was glad I had a decent gear puller. I did a rudimentary calculation and worked out that it took about 3 tons of force to remove the pulley. But everything came apart undamaged. I did take a few photos of the process if you're interested.Best wishes,
Chris