Can you guess what this is?



formatting link
Michael Koblic, Campbell River, BC


piece of scrap metal?

A used plating or derusting electrode?

jsw

It looks like a cooper plate that was used as a backer to weld up a hole.

Close. It is an electro-etching copper cathode left out of solution for 12 hours after using it on brass.

Michael Koblic, Campbell River, BC