The best solution that I know of involves using either a coppier or lazer printer. Make a copy on some paper. Use a clothes iron and iron the copy face side down on the copper. Disolve the paper with water. The trick is to find the best paper. Some one posted here a year or so…

Read the full reply

Hi all,



I have much experience in making printed circuit boards using photoetching techniques. Recently I got 10 Kgs of epoxy glass copper clad boards, double sided, from a friend that quitted his electronics activity.



My past experiences with photoetching have been a great success if I used already-photoresist-coated boards, and a total failure when I tried to apply photoresist via a spray on non photoresist-coated boards (like those 10 Kg of epoxy glass I recently got).



So I wanted to use a different system for these uncoated epoxy glass copper boards.



So far I'm imagining two possible solutions:


1) make stencils, and then spray a normal acid-resistant varnish through its "holes".


2) make stamps, and apply them on the epoxy glass to put a strate of ink where necessary (will it be thick enough?)



I need to produce really fine detail, like 0.2 mm lines (surface mount devices), and these lines must not have any breaks in them, because that would mean an electrical connection break.



What would be the best path to follow, stencils or stamps? I would prefer stamps, ideally.



And, then, what would be the best way to make such a high resolution stamps or stencils?



Thanks! Giovanni


The best solution that I know of involves using either a coppier or lazer printer. Make a copy on some paper. Use a clothes iron and iron the copy face side down on the copper. Disolve the paper with water. The trick is to find the best paper. Some one posted here a year or so ago about the paper that he had found to be the best. Probably wouldn't help you as he was getting the paper in one of the U.S. chain office supply stores.

Dan

Frankly I don't think you're going to get very many 0,2mm (< 8 mil) lines of any length reliably with either stencil (screen) or a toner transfer process. Maybe with a lot of $$ practice. I've found them dubious under 15 mils with my limited playing around with them (usually use a commercial proto service).

Suggest either trying to coat the boards yourself with photoresist (also troublesome!) or go the professional route for relatively fine lines, which is to clean the board then laminate dry-film photoresist to the board. You need a laminator of roughly the right temperature and pressure that can take the 1,5mm or whatever thick boards. Getting the film in < 1 roll quantity is the only trick. Here's one US source:

formatting link
BTW (metalworking content) this method can also be used for chemical milling of thin metal parts.

Best regards, Spehro Pefhany

But - I thought that's what circuit board etching *was*!

:^)

Jim

================================================== please reply to: JRR(zero) at yktvmv (dot) vnet (dot) ibm (dot) com ==================================================

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required