I was struggling trying to face some big 304 stainless mold inserts to length. 1.5" diameter & 1.375" length. Saw cut of course. Parting these off is an exercise in frustration.



For most stainless work I hand sharpen HSS Cobalt bits, but I was struggling with my facing tool and to get decent finish would have to touch it up after ever pass. I guess I could move the grinder over by the lathe (cringe) and set a diamond bench stone on the tool cart, but it was rough.



Now as some of you know a lot of mini lathe users swear by those little



21.51 or 21.52 DCMT diamond inserts. I had one tool with one in a tool holder and I tried it because nothing else was working for me. I finished both ends with a single pass on each end of the last six parts with one insert that looks the same when I finished as when I started. After I finished I started going through my box looking to see how many spares I had. Ummm. Zero. There were two broken ones on the head stock, but no spares.

The finish is decent. I just bought some more that are listed as alloy/stainless. Also another turning tool, and a boring bar that uses them as well. I almost bought a through coolant solid carbide boring bar too, but that will have to wait until the next job comes in the shop.



I don't even think I was using it right. It was a right hand turning tool and I was just face/plunging it into the saw cut end pushing a cone off the middle as it finish. I was amazed at how well it worked with such an aggressive cut and no chatter. I even considered turning up the speed.



Its one of those things. You never see the big boys using those tiny inserts. They always have these expensive inserts on giant tools that make chips that hit the floor with a clank. I don't have a giant lathe, but it does weigh a ton (2000lbs). Its only 3HP, but being a gear head its putting out its full real power (whatever that is) at any speed. I should be able to take a decent chip and not blow up inserts. To be fair the lathe does have a coolant system, but I never use it due to the mess. I tend towards cutting oil.

I know those little bitty inserts work on mini lathes, but I never really used them much on the PM14x40 except where needed to cut a back clearance or something like that. I should know better. They made a bigger depth of cut and bigger feed per rev than other things and there was less heat build up in the part. No coolant. Just a few drops of cutting oil.

I'm going to quit pretending I have a big boy lathe and just go back to everything I learned on the mini lathe that worked.

P.S. While I do not recommend them I made a lot of parts on the mini lathe including paid parts. Not just brass or aluminum either.

I heard diamond

  • works for Ali because it has no solubility for Carbon
  • does not work for irons/steels because the hard tool "disappears" by solution into the iron ?

My apologies. I didn't at all mean something like a PVD diamond coating. DCMT is a diamond shaped insert. Typically your find them coated with TiN, uncoated, and occasionally with TiAlN or AlTiN coatings. My point was these small geometry inserts that work so well in under power under-rigid machines like the typical import 7-8 by 10-16 mini lathe also work on a heavier machine. If the big boy inserts don't work these still do. In this case I was cutting 304 stainless steel. It improved the finish, didn't require sharpening, had less heat input, and did the job much faster net elapsed time.

FYI: I do a fair amount of aluminum cutting, and generally I've found bright sharp uncoated tools do the best job and have the best material removal rate for me and leave a good finish. Diamond was popular when I first started cutting aluminum on machine tools, and more recently ZrN has become the popular coating. I've tried them and the simple fact is a coated tool isn't as sharp. They might work better for larger tools on larger machines, but on middle weight machines with limited horsepower (5 or less) a bright sharp uncoated tool works best for me. For high speed flood coolant makes the tool last without chip welding, but coatings do not. On smaller tools horsepower isn't even a factor as the tool can't take it anyway.

Thx for this detail. Interesting yes certainly. Sorry "got the wrong end of the stick".

I used cutting insert tooling - aagh - 30 years ago. Vertical milling shell-cutter on steel. Did well - they'd never seen steel chip ejection like a chain-saw cutting timber. Took a visit from the rep. who explained this is how the tooling is supposed to be used :-) Coated carbide inserts - coating the gold coloured one - a Ti nitride(?) coating - for this steel.

Pushing it harder and harder. As I once offended Jim a little (sorry Jim) over... time is money. Even if you are doing something for fun, favor, self... time is still your most valuable nonrenewable resource.

I needed to make another batch of stainless mold cores today. (Stock design that uses upto nine (9) 1.5in diameter cores to varY the size of the casting. That's 18 cuts to true them up after they come off the saw.

My new inserts arrived a few days ago ago, but I wantedif I could bump up the speed a bit with that little hobby lathe size insert. I had been using at at 300 RPM in low gear. That's a starting SFM of 117 if I have done the math right. I am sure there are folks pushing big turning centers orders of magnitude faster, but this is after all only a bigger import lathe. Its still an import lathe, and while its relatively heavy, its light for its size.

Of course the SFM drops as the diameter is reduced. Maybe I could go faster if I cranked up the speed as I reduced the diameter, but this is a single phase gear head lathe. The motor just turns one speed. The time to stop it and change gears would eat up any time savings.

Just for the heck of it I decided to see how much faster I could start. At 460 RPM the insert was still doing fine. Still using the same insert I used when I started this thread. I don't mean the same type. I mean the same insert. That means the insert was hitting the outside of the stock at 180 SFM. The number doesn't sound much bigger, but the part time was definitely faster.

A couple ends with an intact insert at that speed and I decided to try the last couple parts at 755 RPM. 296 SFM. That was significantly faster. Part time was a lot shorter, and the insert still looks like when I started. (I'll look at under magnification later) It wasn't so fast that I had any issue keeping up, but it was fast enough I couldn't do anything else, like move the stock in the saw to cut the next rough blank.

Now that I have spares I think next time I cut a batch of these cores I am going to push it until I chip an insert to see just what they will do.

Please bare in mind that these are relatively light cuts. The blanks come off the saw at about 1.4" to 1.41" and get trued to 1.375".

You didn't offend me, I describe what I know best, which is low volume custom work, perhaps relevant to a hobbyist. I haven't done enough production machining to comment on it.

What is the insert? Maybe there's hope for using it on my leather belt antique South Bend. So far except for the GTN-2 cutoff insert of unknown make they have all quickly chipped. I get away with HSS only because it doesn't need to hold size very long. jsw

I've been using a lot of carbide tooling on my 10" Logan since I built the QCTP ... but I'm not getting rid of the lantern toolpost and HSS stuff because thewe are just some things it works better on .

Yep. Any interrupted cuts, anything where you need a really sharp edge (copper,anyone?), anywhere you do not have overwhelming power - inserts are designed for use in powerful machines and don't usually have sharp edges, so need more power than HSS.

Horses for courses. Though I mostly use inserts myself even on a minilathe.

Peter Fairbrother

And I just found out how fragile threading inserts can be ... I'm sure glad I bought extras ! I hope I hit the knee of the learning curve before I run out .

I've been using a lot of carbide tooling on my 10" Logan since I built the QCTP ... but I'm not getting rid of the lantern toolpost and HSS stuff because thewe are just some things it works better on .

-- Snag Illegitimi non carborundum

-------------------------------

I happened upon a Multifix set while searching for a used dovetail type, and like it very much for HSS because of the rotation in small steps. It's easy to set a hand ground bit to both turn and face. Extra Chinese tool holders fit the Swiss post perfectly. Size A is right for my 10" SB. I haven't needed the more compact lantern post in years, a bolt and shim setup is more versatile for turning a ball or socket with the compound.

formatting link

There is certainly something to be said for being able to freehand grind a specialty HSS tool, but for the most part I just put them in tool holders for my QCTP.

I'm actually not 100% sure about this particular insert. It might be a unicorn. I think it came on a tool. I'll let you know how the alloy/stainless inserts I bought work out when I finally destroy this one and have to swap it out.

I think the big deal is that the small insert has to have smaller geometry so it works better when making smaller cuts.

I suppose a lantern tool post "might" be able to hold a smaller scrap of HSS, but to really get the most out of your HSS a tangential holder might be the way to go.

I suppose a lantern tool post "might" be able to hold a smaller scrap of HSS, but to really get the most out of your HSS a tangential holder might be the way to go.

Bob La Londe

------------------------------- I have a good selection of Armstrong and similar bit holders, obsolete

1960s-style tooling that matches my 1965 lathe. It's fine for carbon steel up through Grade 8 bolt hardness and puttering geezer productivity.

I've seen only a few tangential holders for sale, for formed threading bits and priced high. I made one to hold the shank of a broken carbide drill bit nearly upright to turn the race grooves in a stainless thrust bearing sized to fit pipe, for a solar array. My hands are still steady enough to grind a threading bit to closely fit the arrow gauge.

Today's rainy day project is turning closer fitting spacers and bushings for the ball bearings in the sawmill blade guide rollers. jsw

I have freehand ground a lot of things, and I can probably make an adequate threading cutter, but a simple miter gage and slot in a tool rest makes it achievable for nearly anybody. Even a puttering geezer.

I have freehand ground a lot of things, and I can probably make an adequate threading cutter, but a simple miter gage and slot in a tool rest makes it achievable for nearly anybody. Even a puttering geezer. Bob La Londe

-------------------------------------- So does a Univise on a surface grinder, when I want to be fussy. I haven't seen a Baldor carbide grinder for less than $600.

On Sun, 18 Aug 2024 17:02:31 -0700, Bob La Londe snipped-for-privacy@none.com wrote as underneath :

Interesting thread Bob, thanks, is this example the type of tool you are talking about? Never come across the diamond tipped versions of inserts but my original machining in industry experience was in the 1960's! Only hobby level now..

formatting link
says for non ferrous but you are using on stainless without any red spark? Can they be touched up if/when the edge goes? I know its only a single but looks uncheap to me! C+

If you read Bob's post 30/7/2024 he clarifies he's not talking about diamond tipped inserts but diamond shaped rhombic inserts.

I bought a couple dozen HSS blanks, 10x10x100mm, maybe 20 years ago, and still have a few unused ones, and several with cutting ends which I don't use which could be reground if needed. No need to fiddle about with scraps of HSS, though I do have a few home-made toolholders, mostly of the weird and wonderful kind, for them when needed.

For smaller machines I make my toolholders/toolposts, one for each tool, from a 50x50x30mm [18] block of mild steel. I mill a ~14mm slot on one edge, then drill and tap a couple of M5 or so holes into it to hold the tool in place. Then I drill a hole for the toolpost stud.

Add a couple screws, put in place on the rest with the tool, then shim to center and tighten. Then you can change tool-plus-toolpost just using the toolpost handle, and it is a much firmer hold than any other toolpost I have come across.

Ketan (of Arceurotrade) once quite unwarrantedly called me a Hell's Angel for the way I "brutalise" that minilathe (which is still running well 20 years on, though it has had a bearing change. And a main spindle change too, bent it somehow. Motor electronics replaced [47]. Hmm maybe that comment wasn't so far off...

I don't do a lot of bigger stuff, but I do use harder-to-machine materials like inconel, monel, stainless, copper, titanium, hastelloy (ouch) etc.

Also alumina and other ceramics - for which I use the nearly-cheapest diamond tooling, like drills, hole saws, cutting disks, to get back a little towards the title of this thread. Keep them wet, underwater if possible, take your time, be firm but not hard, and they cut like a knife through butter, albeit a lot slower. Accurate on the second cut, and the finish is lovely.

I have also used these on hastelloy, which I couldn't get to cut nicely even with CBN inserts. A dremel in the toolpost is handy. Cheap diamond tools are exactly that, cheap. They don't last that long, perhaps less on steel [99], but if the alternative is waaay expensive or unavailable ..

I never use so-called machinable ceramics, far too expensive for zero gain. If machining ceramics, or using diamond tooling, don't forget to cover all slides and clean the machine immediately, as the dust will kill accuracy.

Peter Fairbrother

Chester minilathe

2x Myford ML10 Myford ML3 extra looong bed Boxford AUD home-made CNC lathe 7 BCAs, one CNC'd Seig X3 mill

[19] 25mm sometimes, but 30mm is better, sometimes 25mm isn't enough.

[49] to repair the electronics on a single=phase brushed DC minilathe or minimill motor, don't bother with the kblc board if fitted, it is a POS. Chuck it. A cheap chinese 180V DC controller from Ebay will do the job, and if it breaks throw it away and buy another. I was doubtful and bought a spare, still have it about 15 years later.

[99] the diamonds come off before they dissolve in the steel. If you are using the expensive brazed ones it might be a problem

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required