These accounts would be interesting. Do you recall where you saw them?
Johannson's patent is from 1907 or so.
For a nice description of how such things were done 100 years ago, see ³Accurate Tool Work², Goodrich and Stanley, First Edition, Eighth Impression, McGraw-Hill
1912, 217 pages. The last two chapters are on the then recently invented Johansson Blocks, with microinch precision .Joe Gwinn