I am new to this welding biz. I am making acceptable welds, but they're globby. So a nice electric 4" grinder can take care of most of this. But what does one use to get into and grind globby welds in tight places, where a 4" welder can't get?
Thanks
Didn't find your answer? Ask the community — no account required.
Back on track welding up all the little short connectors to joining the joists...
J
Jeff Dantzler
I use an old Makita die grinder that I got at a local auction for $5.
However, I try to avoid grinding welds whenever possible. Usually I only grind them for clearance purposes. Sometimes I want to "disappear" them though. A flapper wheel on a 4 1/2" grinder is great for this.
If you give more details on your welding setup, folks may have some suggestions for reducing "globbines".
Jeff Dantzler
B
Burnt Fingerling
It's a Lincoln ProMig 135 that I use. Most of my globs are inexperience and not being used to seeing through the dark welding shield. I use one of the auto darkening hoods, but I still find it difficult to see. Old age, I think.
I am doing this for appearance as well. Just to smooth 'em out. I had a fab shop make me a sissy bar for my bike a few months ago, and it was obvious they made everthing look smooth with a grinder.
I looked at pics of Makita die grinders. Would a Dremel do the same with the appropriate tip? Or is it not up to this?
Thanks, Bob
T
Tom Martinello
A Dremel should work fine for you, if you have the appropriate grinding tips.
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?
Ask the community — no account required
Report Content
You are reporting this content to the moderators. They will look at it
ASAP.