Is it possible to cut a quarter panel off a car with oxy/act?

Nov 24, 2007 1 Replies

First reply

rustyjames

I would use nibblers or a saw. More than likely it'll distort the metal and unless you have the upholstery and glass stripped or protected, you'll run the risk of damage to them as well.

Read the full reply

I know that it CAN be cut but is it possible to actually cut the panel without distorting it so that a patch can be used? I know that an air body saw or plasma is likely best but how would you suggest tackling (if at all) with the torch?



Thanks. Andrew.



I would use nibblers or a saw. More than likely it'll distort the metal and unless you have the upholstery and glass stripped or protected, you'll run the risk of damage to them as well.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required