It must be that infamous 'Texas toast'. ;-)
It must be that infamous 'Texas toast'. ;-)
Shipping container, old step van, basically a big box you can keep dry. As long as the interior space is filled you won't have as much trouble with interior condensation. So a full container will stay drier than a mostly empty one.
As to the wire spools, just bag them individually in tough trash bags, on a dry day. Throw in some handfuls of uncooked rice or beans to absorb any moisture that does get in, and store indefinitely. Best if the rats or mice can't get to the beans or rice. They will chew lovely holes in the bags.
I tend to agree with some of the others that an old refrigerator would work fine. When I was in high school our instructor used an old refrigerator to store our misc. welding rods.
But, with as much as you need to dry, you'll probably need several old refrigerators.
Gunner needs ideas for rod storage and to this I say:
How about A pickup box trailer with a topper mounted on it. If you find someone that wants to buy A few hundred pounds it would be easy to transport it. Another idea would be a dead commercial grade freezer. An upright stainless steel freezer from A restaurant should hold at least 1500# and be easy to find what you want without unloading what you don't want.
Good luck! H.R.
" Aim low,reach your goals,avoid disappointment". Anon.
A walk in cooler?
Plastic buckets with lids could be stacked 2 or 3 high. How heavy would a bucket of electrodes be?
Over 100 lbs. Some buckets can tack that, but others will break down over time under that load, especially if you stack them.
Indeed. So do milk cartons.
Gunner
Are there any good sources of used 55 gal. drums around? Or how about the smaller ~15 gal. oil drums? I'd think you could pick up a bunch for cheap from your customers. As long as they still have the lid I'd think they would work very well -- heat up the rod to drive off moisture, dump it in, seal it, and label it.
Here's a few ideas for doing it cheap: tie it up in ~15 pound bundles and wrap it with aluminum foil, and then dip it in wax or spray it with something similar.
Vacuum seal in plastic bags and store in old foot locker. You might even get a sheet of mylar and make your own bags for cheap. I think all you'd need is a iron, or a bit of nichrome wire. Harbor Freight sells a bag sealer, too.