SAW

Aug 26, 2008 1 Replies
Jump to replies (1)

what is the W/d ratio for saw welding



whether excess penetration is good for fillet welds say ...circumferential fillet welding of thickness 12 mm rim and



36 mm inner disc the root penetration exceeds about 6mm and fillet size is 8 mm and throat is 5.2mm

pls give ur suggestions


mm rim and

8 mm and

Typical depth to width ratio in sub-arc welding is 2 to 1. That is the depth should not be more than twice as wide as the face. More than

2-1 leads to internal stress cracks. phil

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?