WELDING OF MARAGING STEELS TO AISI 4340 STEEL

Apr 30, 2004 0 Replies

SIR



CAN ANYBODY HELP ME BY SUGGESTING THE APPLICATIONS OF DISSIMILAR ALLOY WELDS OF MARAGING STEELS TO AISI 4340 STEEL



I USED FRICTION WELDING FOR THIS



SUGGEST ME SOME MATERIAL AND WEBSITES REGARDING WELDING METALLURGY OF MARAGING STEELS



FINAL ONE IS MANGANESE IS DIFFUSING FROM 4340 STEEL TO MARAGINGSTEEL IN THE ABOVE WELD WHICH DRASTICALLY AFFECTING THE NOTCH TENSILE STRENGTH OF THE WELD. CAN ANYONE HELP ME THE REASON FOR THIS



THANK U