I seek the thermal properties of liquid raw latex as tapped from the tree.
- freezing point
- heat of fusion
- specific heat capacity of the liquid
- specific heat capacity of the frozen solid
Serious google-ing hasn't helped. Anyone know which trade association libraries might have this info at hand?