It is not true that there is nothing good on the web. There are a dozen web pages originally from either books or magazine articles floating around as Acrobat (.pdf) files that can be downloaded, either directly from ASM or elsewhere.



Six of these are from the magazine, "Practical Failure Analysis", which recently was renamed with the broader title of the "Journal of Failure Analysis and Prevention".


  1. "Techniques of Failure Analysis," Chapter 1 from the book, Understanding How Components Fail, 2nd ed.by Donald J. Wulpi,
    formatting link
  2. R.A.Lund and S. Sheybany, ""Fatigue Fracture Appearances"" section from the ASM Handbook, Vol. 11, Failure Analysis,
    formatting link


  1. Randy K.Kent, "Uniform Corrosion," section from the ASM Handbook, Vol. 11, Failure Analysis, pages 767 to 771,
    formatting link

  2. Randy K.Kent, "Intergranular Corrosion, section from the ASM Handbook, Vol. 11, Failure Analysis, pages 777 to 785,
    formatting link


  1. Colin Sandwith and Randy K.Kent, "Velocity Affected Corrosion, section from the ASM Handbook, Vol. 11, Failure Analysis, pages 788 to



795,
formatting link

  1. Rodney Dean, ""Legal Issues Involved in Failure Analysis,"" Journal of Failure Analysis and Prevention, April 2004,
    formatting link


  1. C. Sly, ""Counterfeit Parts: The Scourge of Industry,"" Practical Failure Analysis, August 2001,
    formatting link

  2. D. A. Moore et al., "Crankshaft Failure and Why it may Happen Again", Practical Failure Analysis, Vol. 1 No. 3, June 2001, pages

63 to 72,
formatting link

  1. M. E. Stevenson et al "Metallurgical Failure Analysis of Titanium Wing Attachment Bolts," Practical Failure Analysis, Vol. 3 No. 4, August 2003, pages 75 to 80,
    formatting link


  1. R.J.H. Wanhill, "Faiilure of Backstay Rod Connectors on a Luxury Yacht," Practical Failure Analysis, Vol. 3 No. 6, December 2003, pages 33 to 39,
    formatting link

  2. P. C. Chan and J. C. Thornley, "Common Features of Fretting-Fatigue Cracking in Steels," Practical Failure Analysis, Vol.

2 No. 6, December 2002, pages 85 to 90,
formatting link


  1. A. Crosky, "Failure of a Fairground Ride," Practical Failure Analysis, Vol. 3 No. 1, February 2003, pages 48 to 54,
    formatting link



Pittsburgh Pete


formatting link

Thanks for the continuing effort to post these links.