I don't know if this is the right newsgroup for this kind of questions. But I wished to ask you which type of steel is better for a sword. Naturally considering the relationship between weight and 'hardness'.



Thanks in advance,



Using steel, weight depends almost just on geometry. Maximum hardness depends mostly on carbon content. But you need toughness as well.

Michael Dahms

Just a couple weeks ago my metallurgy instructor was asked- "which stainless steel would be best for a sword?"

"as a wall hanger or what?"

"no, it needs to be able to handle some sword to sword hits"

I butted in and said- "none of the above!:)" (I'm your basic stainless steel hater)

The metallurgy instructor laughed and said- "in that case 4360 made of lower bainite"

I butted in again and asked- "where in the heck do you get 4360?" "how about L6 (4370) that can be had from Admiral Steel for cheap, would it be as strong as 4360?"

"yep, just a little harder is all"

Any comments? (your chance to butt-in;)

Alvin in AZ ps-

formatting link
it sez the L6 is 3/16" thick but it's really .224"

try this:

formatting link