6 Pin Connector

Apr 27, 2007 1 Replies
Jump to replies (1)

Can anyone provide a wiring diagram for the "male" half of the connector specificaly for a remote amperage control? I have the diagram for the welder (Lincoln V160S) Feel free to PM me.



Sorry to be so slow to reply. If all Lincoln welders are the same, then A is one side of a 10k pot. B is the wiper. C the other side of the pot. D and E are to arc start switch. F is unused. Next time ask on sci.engr.joining.welding

Dan