Aluminum flatbar axle strength?

Aug 22, 2016 2 Replies

First reply

clare

A little more than the weight of the scooter - Perhaps it might hold a 5 year old

Read the full reply

How much weight will this 21 inch long 0.375" x 1.25" aluminum flatbar axle support?



formatting link



Personally, I am not concerned about the center joint. It is a bottom bracket that can withstand lots of twisting force from bicycle cranks and pedals. The flatbar will be firmly attached.



I would rather make a two wheel vehicle, but I live in a nanny city that prohibits power assisted scooters. They probably do not enforce it, but you never know. So I am making a motor assisted tricycle.



Thanks.


A little more than the weight of the scooter - Perhaps it might hold a 5 year old

couple dozen pounds.

Firmly attached until it breaks off that is.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required