I recently went through some iterations making a wire bending tool for a customer.  I sheared some stainless dowel pins in testing.  Then I tried some alloy steel dowel pins and made a series of test bends with material and applications far hard than the customer claims he's doing.  The customer managed to shear one of those.  Finally I went to high speed steel drill blanks.  Close tolerance set in Loctite 640 cut just barely long enough to do the job to minimize leverage against the pins.  The math says I have a fair safety margin.



Of course HSS drill rod doesn't come in nice convenient standard dowel lengths so I had to cut the pins with an abrasive tool.  A little fiber Dremel disc on a rotary hand piece.  Of course that leaves a burr which I ground off with a diamond conical point, but the diamond reacts with steel at grinding temperatures and of course only lasted long enough to deburr a few pins.



It seems that small rotary grinding points exist in a conical with CBN, but actually finding them for sale is being a bit of a struggle.  McMaster seems to have no small CBC grinding points, and Penn Tool only has cylindrical.



Of course I sent one replacement rotating assembly off to the customer (4 pins its double ended) and then I finished one for myself.  I would like to make small batches of these for customers, but I don't want to have to replace a diamond conical grinding point after every few pins.  who actually stocks them online?  Searches just keep coming up with diamond.  I don't want diamond.



A 1/4 inch conical with a 60 degree point and an 1/8 inch or 3mm shank would be ideal, although I do have a few rotary hand pieces with 1/4 inch collets as long as the grinding point isn't so big or gets in its own way or blocks my view while working.


I've read that diamond can survive grinding steel as long as the surface speed is below 3600 (or 4000?) SFPM. Perhaps that's how they last on a Drill Doctor.

Dremel universal brush motors can be slowed down with a Variac. I haven't tried a lamp dimmer.

You telling me to keep my foot off the pedal?

I found a CBN conical grinding point finally. It's a little smaller than I wanted, but that's better than to big. They aren't cheap, but in my searches I found conical grinding points (all cylinders) that cost a lot more. They are not particularly expensive either. If they work, it's not cost prohibitive.

formatting link

My small lathe accepts a 1/2" Jacobs chuck with a 1/2"-20 thread mount directly and I made a 1.5"-8 to 1" collet adapter for my big lathe for a larger Jacobs lathe drill chuck. The aren't ideal for turning but can hold any size round or hex in their range for filing, grinding and polishing.