My latest domestic kitchen-support project was to take a very stiff



12"x18" high-density polyethylene (HDPE) cutting board, and trim it down to 17.5", so it fits snugly over the stainless-steel kitchen sink, allowing my wife to cut messy foods over the sink (and disposal).

Trimming the cutting board was easy with bandsaw and an ordinary woodworking plane. The machining part of this project took maybe 30 minutes, mostly due to trimming and rounding edges with the woodworking plane so the board rested snugly and securely on the edges of the sink.



For the record, ordinary (low density) polypropylene is a bit too flexible, even if 0.5" thick. (The board cannot be thicker than this and still fit in the dishwasher.) I was looking for 0.5" polypropylene, which is offered by such web merchants as chefscatalog.com (Item #



24406), but The Container Store claimed to have such a thing, and they are local, so I went there. It turned out to be 3/8" thick and made of HDPE, not polypropylene, but seemed stiff enough, and cost only $17 or so. The Chef's Catalog description is "high-density polypropylene", which does not exist, so I bet it's HDPE as well.

If this modified 3/8" HDPE board doesn't work out, I'll buy some 0.5" polypropylene stock and make a cutting board to fit the sink; this was the original plan.



Joe Gwinn


I think I paid Port Plastics about $20.00 a year or so ago for a 3/4 x 18 x

24 piece of uhmw

--Mostly I use it to divide beef primal sections into smaller roasts, steaks etc....Generally I just wash it by hand although it will fit diagonally upright in the Hobart undercounter sanitizer unit if I use a peg style plate rack.

The trouble with plastic cutting boards is that they look like crap in short order and the wounds in the plastic harbor nasty critters. Consider laminating some hard Maple strips then machine. It will look good and last forever.

For my Bosch dishwasher, 18" by 12" by 0.5" fits nicely along one side, leaving the rest of the space for dishes.

I did try to use a piece of 3/8" UHMW polyethylene as a cutting board, but right from the start it would not lay flat on the counter, so it was withdrawn from the kitchen, and now serves to keep my 4-jaw lathe chuck up off the concrete floor.

Joe Gwinn

The dishwasher does a decent job of keeping the critters out of the gouges. The real restaurant supply places sell thick 3/4"+ plastic cutting boards that are intended to be belt sanded now and then when they get gouged up. Personally I use a bunch or the thin flexible plastic cutting boards and like the ability to flex them into a chute when depositing the items I chopped on them into a pan or bowl.

Which is exactly what I did - twice . Once for the kitchen sink at home , once for the little double sink in the camper. Good use for scrap , and I've made several for wedding gifts . The newlyweds loved 'em . Use Gorilla Glue ...

I must say that I prefer wood, but my wife prefers plastic for all but cheese. So, plastic it is.

Joe Gwinn

Machine sand with 220 - 320 grit to remove the scratches.

Man, Scarysharpen your knives and stop cutting into the boards so hard. They last forever!

-- Woe be to him that reads but one book. -- George Herbert

"Joseph Gwinn" wrote

(The board cannot be thicker than this

What do you butcher that is not cleanable by normal means in hot soap and water?

Steve

(...)

Every couple years, I go to my plastic monger and buy several sheets of thin HDPE in various colors. I slice them up into disposable cutting boards and store them in the kitch.

Just like you, I discovered that I could easily form the surface into a funnel and dispense sliced whatever on to a pan or pot.

Rinse it off in hot water and flip it over when one side gets too ugly.

Toss it when both sides are no longer pretty. Cheap, convenient and easy.

--Winston

Every so often I lay towel that's been wetted with soapy water and clorox onto it for about 10 minutes.

(...)

I stumbled across this just now from:

formatting link
"A good procedure for disinfecting both wood and plastic cutting boards, as well as other surfaces and utensils, is to spray them first with a mist of vinegar, then with a mist of hydrogen peroxide."

I don't know what the vinegar is supposed to do, but I am a real evangelist for the power of H2O2, especially the "40 volume" (12%) liquid (non cream) stuff. That *smokes* microbes RFN.

formatting link

--Winston

Turn it into a sideboard top, preferably Mission style.

-- Woe be to him that reads but one book. -- George Herbert

Winston fired this volley in news: snipped-for-privacy@news4.newsguy.com:

That's all the MORE reason to "get exposed" to minor amounts of infectants.

When I went to RVN, I was a "country boy". NOBODY would eat anything the locals serve, for fear of getting the runs.

I ate everything I could buy, and suffered greatly for about a month. After that, I could eat off the local economy any time I wanted, without penalty.

Gotta build up the "gut bugs". It's actually MORE healthy than surviving in a sterile environment.

Hell... I even (still) keep (and use) a bottle of Nuc Mam in the pantry. It's good, if you can get past the smell!

LLoyd

It's all fun and games until you come down with a case of misdiagnosed MSRA:

formatting link

Who said anything about 'sterile'? :)

--Winston

Indeed. Same here. Though I still dont much like nuc mam.

Gunner

Whenever a Liberal utters the term "Common Sense approach"....grab your wallet, your ass, and your guns because the sombitch is about to do something damned nasty to all three of them.

Precisely.

Good call. You realize that tourists to the USA get the trots, too, right? It's all because we have different intestinal bacteria in our food and water.

Rightio.

Fish sauce? Ewwwwwwwwwwwwwwwwwwwww! Humming "Fish heads, fish heads, lovely little fish heads!"

-- If we attend continually and promptly to the little that we can do, we shall ere long be surprised to find how little remains that we cannot do. -- Samuel Butler

Keep researching it. You'll find some real docs concurring.

It keeps the skin from healing back together as rapidly and causes more scarring.

"Hi. I'm Joe Blow. I'm from Nawlins. I live in a city which is built on ground UNDER sea level and UNDER the level of the lake next door." Pay me when it gets hammered by a hurricane or the river overflows or the lake overflows onto my land. I'm a victim. Pay me NOW!"

-- If we attend continually and promptly to the little that we can do, we shall ere long be surprised to find how little remains that we cannot do. -- Samuel Butler

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required