I just bought a nice used baldor 10 inch grinder (3PH). It came with some well used 8 inch wheels. Looking for advice on what kind of grinding wheels to put on it. I will use it mostly for grinding HSS toolbits.



I think this grinder came out of a school, so they may have put 8 inch wheels on it just for economy or they may have desired a lower surface speed. One person recommend a 10 inch wheel for roughing and an 8 inch wheel for finishing.



When it comes to grinding wheels I belive it buying the right one the first time. It does not pay to skimp.



thanks chuck


I use 46 grit K grade 32A and 60 grit K grade 32A pink aluminum oxide wheels on my Baldor, which is used almost exclusively for sharpening HSS. The hard gray wheels that were on it didn't work well with HSS. Remember, the softer the material, the harder the wheel and vise versa.

Grant

Charles A. Sherwood wrote:

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required