Hello Quite a number of you are good with electronics. Welding machine - MIG, for Ali - took it back to manufacturers - did the several hundred mile journey. Spent an entire morning in tests. I did the weld runs while testing conditions.
I developed a tentative hypothesis
- that the "wire-feed-speed" control actually sets an aim Amps - that is what the readout is saying - and when the wire-feed and arc starts it tries to "fly-by-wire" to the set current - and does it badly... Reasons for conjecturing this
- the starts are faltering on both CV-MIG and CC-SMAW (going with no calibrated "initial" condition it takes too long to work out what it should be doing)
- changing wire diameter while leaving the "wire-feed-speed" adjuster ("pot.") has nothing like the effect expected on the Amps - going from
1.2mm to 1.6mm wire the current goes-up about 9%, where if the wire-feed-speed stayed the same, the amps should go up by 78%
[that "78%" is geometric - 1.6:1.2 = 4:3 diameter = 4sq:3sq area = 16:9 ; = 1.777recurring ; 1.77. - 1 = 0.777. -> 78%]
I have met expensive "super-industrial" MIG machines running on 3-phase where one option is to set Voltage and Current and it presumably does "fly-by-wire" to make that so - and do it well. Done flawlessly - it is a time-saver for a busy welder-the-person. But anything is imperfect - back to Volts (reasonable to set the aim on that) and wire-feed-speed...
What was found in those 3 hours of testing (no-one at the welding machine Co. can do Ali-MIG welds) is...
It does do fairly alright (there are caveats) when rigged with 1.2mm wire (is "5356" Al-Mg)
But put in 1.6mm wire and there is a rough noise, aluminium sprays around, there's white smoke (fumed Ali?) and loads of black "sooting" on the ali plate (fumed and condensed Mg ? certainly) - while what is deposited is a mess which could never be called a weld...
I have made angling at "consumer law" in the UK
- with 1.2mm wire the GMAW-gun / MIG-torch "craps-out" in about a minute or two of welding - by overheating whereas "as expected" the torch sustains with 1.6mm wire
- with a 410A machine - 100% ie. industrial application duty at about 280A - there is no way this machine can viably run 1.2mm wire *only*
- the Lincoln Foundation conditions, "the bible" - their "Table 9-13" in 14th Edition - which have been there unchanged for at least 6 decades - and probably were arrived-at in the late 1940's - all say 1.6mm wire (1/16th-inch), increasing to 2.4mm wire (3/32nd-inch) at 240A plus - ie. "the bible" says; don't even think of arguing
Anyone able to make any sense of
- the welding conditions (I know I have risen to the status that many defer to me on these matters)
- the electronics and control (what I take you to be the experts on)
I am thinking of telling them - taking it that the "pot." sets "fly-by-wire" aim Amps - that this machine is not sophisticated enough to "pull this off".
So they need to get "pot." sets wire-feed-rolls revolution rate - which has only one "calibration line" - so the rolls can get going per calibration relationship - and if there is any "fly-by-wire" it is to monitor the revolutions rate in some way and nudge it to the set-point always despite changes in friction with bending the "harness" (hose/cable) around corners, etc.
With a water-cooled torch/gun, with 1.2mm wire the 14m/min (550ipm) upwards wire-feed-speed with 1.2mm wire can be sustained.
HOWEVER - even if they were to FOR FREE (which would be over US$1000 value if purchased) fit the machine with a water-cooler and give me a water-cooled torch/gun I would not be entirely happy, because the setup is much more desirable, and what you do not want is to come back from having a pee and finding your own machine is gone...
If the machine is owned by the employer; no - that machine comes back else people get "fired". Hence water-cooled-torch pulse-electronics machines at sites owned by the site owner.
The air-cooled one is a "<no polite description>" machine of low value no-one could sell - who would buy it?! - and it would "stand-out like a sore thumb" - so one could take it to sites to do "contract" work.
Can anyone make any sense of any of this?
I will write my message to the maker of the machine now, and look out for responses in a few hours towards the end of our Sunday here in Britain.
Regards to all, Rich Smith