Feb 24, 2012 19 Replies
Jump to replies (19)

I need to make a pin .25" long by .096" diameter with a 0.109 by 0.117 head. It needs to be hard so I'll make it out of a 7/64 drill bit, the size of the head.



What's a clever way to hold this in the lathe? it would be hard to make soft jaws go down this small. I'm thinking some sort of collapsible bushing that I'd drill.



Karl



How about drilling a hole in a piece of round stock with the 7/64 bit. Then gluing the bit in the hole. Mount the piece of round stock in the chuck and go to work.

A split sleeve - something like a collet?

Like one from a Dremmel tool?

Once you get it made, how do you harden it without burning it up?

Paul

Can you use 5C collets? If so, consider getting an "emergency" collet, soft, which can be drilled/bored to size.

Or -- if you have a small enough lathe with a Watchmaker's spindle, you should be able to find a WW series collet of just the right size. For the 0.109 (if that is the diameter), a #27 or #28 collet (they are marked in tenths of mm). For the 0.117 (if *that* is the diameter, you would need a #30 likely, or perhaps a #29. (It calculates out as 2.9718mm FWIW.

The WW collets are one of my reasons for holding on to both my Unimat SL-1000 (with the watchmaker's spindle), and the Taig (with a similar but less versatile spindle).

Good Luck, DoN.

Paul Drahn fired this volley in news:ji74af$glc$2 @dont-email.me:

Wrap it in stainless steel heat treating wrapping foil first. And start the process in a carburizing atmosphere.

LLoyd

Regards,

Boris Mohar

Got Knock? - see: Viatrack Printed Circuit Designs (among other things)

formatting link
void _-void-_ in the obvious place

Seems simple for a smart guy like Karl so I must be missing something but here goes anywar: I would make it like this

Chuck up a piece of 0.25 drill rod (O-1) in the late 3 jaw chuck with

1/2 inch extending out

Cut the diameter to 0.109 by 0.357 long

Cut down to 0.096 by 0.25 long

It is going to spring a little so use light cuts to finsh it off

Part it off

Heat treat by placing it on an SS plate and heat from the bottom

I made several pins this way with even smaller diameters

What am I missing? Why not a 7/64 collet?

They do make pin vises for such things, chuck it up in that, then center it up in the 4 jaw. And drill shanks are soft and you'll have a hard time hardening it if the bit is HSS. Go get a piece of drill rod the right size, the good stuff comes with heat treatment instructions so you can get the proper hardness. You could almost chuck the thing in an electric drill and reduce the size with a file. There's not that much to take off. Make two while you're at it.

Stan

Stick it in a drill chuck. You could grab the drill chuck in the lathe chuck or maybe fit the tailstock chuck to the spindle with a live-center sleeve.

Jacobs ball-bearings chucks work pretty well on a lathe spindle. I leave a 1/2" 33B on my 6" lathe and have a 58B on the indexer, and made an adapter to fit it to the South Bend.

formatting link
In one of their pamphlets SB says the chuck was meant for refinishing automotive valves and shouldn't be used for heavy turning.

jsw

You made me curious so I went down to check. 1/8" music wire in a 5C collet cuts easily with HSS, ground to a sharp point to make a square shoulder.

jsw

Doh! This is how I did it. Sometimes i have a brain fart.

I've got 2J collets for my 10EE but not many real small ones.

Karl

Mabee something like a pin vise?

If this is a onesie job, and if there are some standard collets available, the way I do these things is to wrap steel or copper wire aound the shank until it fits in a standard collet. You can only use a single layer, of course.

Otherwise, I turn a sub-collet from anything available and split it down one side. I've tried splitting them part-way down, with two or four slits, but the end result doesn't seem to be any better.

Someone mentioned that the shanks of drill bits are soft. That's quite accurate. Also, they aren't any specific dimension. They're smaller than the nominal diameter of the bit. Sometimes, they aren't very round, either.

Oil-hardening drill rod is the ideal material. But you could also make them from mustic wire. It's going to be quite hard, but it's plain-carbon steel, so you can anneal it over a kitchen range or (carefully) with a torch. Then it's easy to heat-treat, heating quickly and quenching in oil (it's so small that there's no need for water). Just don't soak it at heat or it will be brittle as hell, from coarsening of the grain, and you'll de-carb the part. Then temper at

350 - 425 F in a kitchen oven, for an hour or so, to get maximum strength.

Note that most drill bits have a soft shank and a HSS blade, so the shank won't do much for you. I don't think that it has enough carbon to harden well at all. (If you only need the surface hardened, you can get some Kasenite or other case hardening pack material for heat treating it.

Good Luck, DoN.

Don't case-harden HSS. The shank has plenty of carbon -- and chromium, and probably molybdenum, to harden it up to over Rc 60.

However, it's not a good idea to do so. There are too many other things going on with HSS alloys; you risk winding up with a weak part unless you have good temperature control.

Note that a heat-and-quench hardening will harden HSS, but it won't make it "high-speed." HSS requires a two-stage heat treatment in order to develop red hardness, and the second stage is a solution/precipitation hardening that is a real challenge in a home shop. It can be done, but you have to know what alloy you're dealing with and you have to know just what you're doing. You also need *very* good temperature control.

Music wire or oil-hardening drill rod would be much preferred. They can be easily and reliably hardened and tempered.

Are you saying that the shank of a typical drill bit is also HSS? I've always understood them to be mild steel welded to the HSS which implements the flutes and other cutting surfaces.

I was assuming that if he used the shank, and had to harden it, it would be mild steel, not HSS, so I was not advising case-hardening HSS.

And it is likely that *if* the shank is really HSS, you won't be able to machine it anyway, unless with a toolpost grinder. :-)

Not at all what I was advising.

Agreed. Much better choices than old drill bit shanks.

Enjoy, DoN.

Yes.

I've never heard that. As far as I know, they just partially anneal the shank, or maybe they don't quench the shank in the initial heat-and-quench.

You can mill and turn annealed HSS. I've done it in my SB lathe, with HSS lathe bits.

That is, assuming the shanks of HSS drill bits are HSS. I'm pretty sure they are, Don. I've never heard of them being welded. I would think that would be an expensive way to make a dtill bit.

Before we leave this, we should point out that most grades of HSS have

*very* high carbon content -- 0.80% to 1.1%. That's up there in the range of music wire and antique straight razors. You won't increase hardenability by treating them with Kasenit. They already have all the carbon they can use for hardening.

The problem with heat-treating HSS is that the alloy constituents that form carbides (there are several) have to be heated just right or you get variable results when they either 1) got back into solution or 2) form free carbides. Without excellent temperature control and timing, including temperature ramping and soaking, you get unknowable results, with a strong possibility you will make the material brittle and weak.

So it's not a material to heat-and-quench with a torch, unless you're willing to experiment.