[SOLVED] Is there anything that keeps molten lead from sticking to metal? (2025 Update) Solved

Dec 30, 2004 Last reply: 1 year ago 21 Replies

Solder resist aka solder mask. Remove with methylene chloride aka dichloromethane or paint stripper. You can also get peelable aka temporary resist.