The undercoating I sprayed on the wheelbarrows that didn't do that (so far) is TMP Rubber Soundproofing Undercoat from Taylor Made Products. The wheelbarrows see only rainwater and condensation, not road salt. There may have been a residue of LPS-3 in the surface rust before I sprayed the undercoating. jsw