Silly Setup

Aug 24, 2024 Last reply: 2 years ago 6 Replies
Jump to replies (6)

Silly setup, but it worked.



formatting link


Something like this ER11 R8 collet chuck might have been better,

formatting link
but the crazy setup did work. In fact this is the third time I have made a mold using this setup with cross pins.

I actually have an R8-ER16, but the collet nut didn't give me enough clearance to do the job.

My current silly setup is a 1/2" piece of steel plate bolted to a faceplate . It will be a fixture to hold a connecting rod so I can use the lathe and my dremel fixture to open up the wrist pin hole . This is part of the Arctic Cat 600 to 660 performance upgrade . That boy is gonna kill himself ...

No matter how sketchy the setup, just make sure it can't break free and chase you across the room, because I can guarantee if it does you will not out run it.

Silly setup, but it worked.

formatting link
La Londe

-----------------------------

I have a similar problem that may end up looking like yours. The sawmill blade guide rollers are 2" cylinders with R8 bearings recessed into each side. The bearings press in with light to moderate pressure and are retained by the center bolt and a spacer between the inner races.

The less-than-$1 import bearings I bought don't hold up too well at the

50~60 MPH blade speed, sawdust spray and varying and unmeasurable blade pressure, so they need to be replaceable. Some come out without much fuss, others need persuasion that's difficult to apply.

I'm considering angled tapped holes that let a screw press on the outer race from its back side. My BS-0 indexer is too tall for the Clausing mill when turned upright, so right now the likely candidate setup is a small 3-jaw on a Morse #2 arbor in my rotary table. The chuck could hold a bearing to align the drill with the outer race plus a second bearing above it on the spacer and a shaft to set the table tilt for clearance, then hold the roller in the same alignment by the bearing recess. Mickey Mouse is alive and well and living in my basement.

I worked with a real Mickey Mouse once, he had played the character in Orlando. He was a skilled craftsman.

I went ahead and ordered an inexpensive (cheap) one of these.

formatting link
Even if its not fantastic and wonderful its got to be better than an 8mm x 120mm straight shank. It might even get here as I am finishing this batch of molds. LOL.

... or it might be a waste of time if the tool holder nose is to close to the spindle nose or quill shoulder. I guess I'll just have to wait and see.