I have need of stainless for various applications and to be frank the local stores just don't stock much. The box stores have a modest selection, but its all no grade listed Hillman crap. Their stainless is worse than their packaged screws if that's possible.
I would like to have some idea what to search for for grades equivalent to steel grades. Like what stainless bolt would I look for to be roughly equal to a grade 8 steel bolt? A grade 5? Never mind grade 2. Like I said, "the box stores have Hillman crap."
Didn't find your answer? Ask the community — no account required.
I would either switch out my gas mix for pure argon and my wire for whatever...
B
Bob AZ
Bob
McMaster-Carr. mcmaster.com
Bob AZ
B
Bob La Londe
A search for "grade 8 stainless" on their site only shows hex nuts. In the suggested search items it shows 18-8, but does not say if that is the same strength as Grade 8 bolts.
E
Ed Huntress
It's not. Not even close.
I think that a Grade 8 in stainless is one very special bolt -- either a
44X-series or a precipitation-hardening grade.
B
Bob La Londe
I did find some reference in a UK welding group that seemed to indicate that A4-80 was close, but the only bolts I've found in that so far are metric.
E
Ed Huntress
Aha. Here's a precipitation-hardening bolt (17-4 PH) that claims to be as strong as Grade 8:
formatting link
There appear to be many others, including 400 Series quenched-and-tempered, but cast a skeptical eye. A Google search on "high strength stainless fasteners," without quotes, turned up a bunch of sources.
There's also a standard for them -- ASTM F593 -- that relates the strength of stainless fasteners to those of carbon and alloy steels.
N
Ned Simmons
You can get 17-4 PH stainless fasteners from McMaster that have approximately the same tensile strength as grade 8 screws. Only $7.06 _each_ for a 3/8-16x1 hex head cap screw. Even MIL spec 18-8 and 300 series stainless fasteners have approximately the same tensile strength as grade 2 fasteners. There's probably nothing wrong with the "Hillman crap."
D
David Billington
IIRC A4 is 316 and those fasteners won't be anywhere near a grade 8. I've seen someone recently confuse metric 8.8 designation with grade 8, a big difference. An 8.8 fastener is about the same as a grade 5.
B
Bob La Londe
LOL. All Hillman stuff unless labeled otherwise is grade 2 or worse. (mostly a lot worse) As somebody who has been shooting screws my entire life for various applications I never saw so many broken screws until Hillman started dominating the market with their "we will fill it for you" marketing. Its easier for resellers, but point blank package screws were a lot better quality 20 years ago.
B
Bob La Londe
Ok.... now I have my two grades. LOL. 316 is about Grade 5, and 17-4 is about Grade 8. I am guessing the 316 would be full hardness to make grade 5 since it's a work hardening spring steel stainless.
Thanks guys.
N
Ned Simmons
A typical 316 SS screw has a tensile strength comparable to a grade 2 carbon steel fastener, around 70,000 psi.
B
Bob La Londe
So are you saying that 18-8 which is a the most common stainless hardware is even lower strength than grade 2?
B
Bob La Londe
Now according to this chart 18-8 is about the same as grade 5.
formatting link
From what I have seen 18-8 is supposed to be the most common stainless for bolts, but that means the stuff at the local boxes must be something else because it breaks a lot easier than a grade 5 bolt. Which is what started this conversation.
Sigh. Back to square one.
B
Bob La Londe
This person claims some, but not all 316 bolts are close, but slightly less tensile strength than grade 5.
formatting link
N
Ned Simmons
I'm saying I don't think you can count on common 18-8, 304, or 316 fasteners to be any stronger than grade 2. Individual lots or samples may be either side of grade 2's, but absent some sort of spec beyond a simple material designation, there are no guarantees.
E
Ed Huntress
formatting link
>
"18-8" is a generic name for basic austenitic stainless steel -- something like 303 - 304, but not necessarily. It is not a technical specification, only an indication that it contains 18% chromium and 8% nickel. The rest of the alloy is up for grabs.
When you see 18-8 used to describe kitchen utensils or flatware, you know only that it's basic stainless. If you see it used to describe fasteners or other technical items, you know either that (1) the seller doesn't know which way is up; (2) the seller doesn't know what the hell the material is; or (3) the seller knows what it is, but it's so bad that he doesn't want to tell you.
E
Ed Huntress
formatting link
It depends entirely on the degree of work-hardening applied to the bolt, and there is no standard for designating it. Annealed, 316 has about 30 ksi yield and 75 ksi ultimate tensile strength. (weak for steel) Cold-drawn wire runs up to 95 ksi ultimate tensile. When you make a bolt from it, it's generally cold-headed and roll-threaded. The strength varies all over the bolt because of the uneven cold-working.
You can't heat-treat 316, except to anneal it.
Hi-strength stainless bolts are made from heat-treatable grades, either
400-series (such as 420 or 440), or precipitation-hardening grades (17-4 PH). You can harden 17-4 PH close to 200 ksi tensile. They cost a bundle compared to ordinary bolts.
B
Bob La Londe
formatting link
>
Thanks. Sometimes a "Grade 8" is the bolt for the job, and sometimes a "Grade 5" is better. I was hoping to find an equivalent for both, but that seems to be not practical. Grade 2 is rarely the best choice except as a shear bolt on farm equipment. Looks like I have the choice of going with quality (ARP) or unknown when it comes to stainless but no other way to grade.
E
Ed Huntress
formatting link
>>
Stainless presents one issue that may or may not be important in a given application. The issue is elongation; when weaker bolts are better in an application, it's usually because their greater elongation -- their ability to stretch, plastically, or to bend -- is important because of the nature of the load.
Austenitic stainless -- the 300 series -- is not very strong in terms of ultimate tensile strength, but a combination of good basic elongation, combined with pretty extreme work-hardening ability, produces a very big spread between yield strength and ultimate tensile strength. This can be very useful in those applications where a bolt may be overloaded and should yield, rather than break. A slightly bigger bolt of a weaker material may substantially outperform a smaller but higher-strength bolt.
The hardenable grades of martensitic (400 Series) and precipitation-hardening stainless *can* have very good elongation, but you have to check the specs on specific grades if it's an important issue for you. The elongation of regular alloy steel bolts is well-known and widely published, if you want to compare them.
Otherwise, it's mostly a matter of how much money you want to spend for the sake of corrosion resistance.
C
Cydrome Leader
agreed.
compare any old stock box of fasteners to what you get a home depot these days.
Hell, even even for bulk wood bolts, I have to hand sort the stuff a high percentage is just deformed.
S
stans4
With stainless, you can have corrosion resistance or you can have strength, just depends on what you really need. And if you need decorative with strength, look for chrome or nickel plate on a regular steel bolt. If you really need corrosion resistance with strength and a real properties sheet, you'll probably end up with aircraft-grade bolts from a real aircraft hardware supplier and also a government-level price tag. They'll probably have ground threads, too, along with more exotic alloying elements. If you gotta have them, that's one place to look. Hardware store stainless is just to plug holes and not rust in a year or two. Also to look hi-tech and shiny.
Re "18-8": That's a very old term for stainless, usually plastered on tableware and kitchen utensils. Not hardenable and about the lowest level of strength. Also non-magnetic. If you're fixing pots and pans, that would be fine. Going to hang off of it 20 stories up, not so great. Not a designation for any sort of mechanical properties.
Stan
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?
Ask the community — no account required
Report Content
You are reporting this content to the moderators. They will look at it
ASAP.