Has anyone attempted a rust repair on a unibody frame.


More importantly, has anyone who's has attempted to repair a unibody (it doesn't have a frame) survived the accident when the repair failed?

yes and i have more to do once the bloody snow melts the biggest trick and concern is to weld to as much structure as possibleto give the repair some meat to stick to. toy have to almost expect the patch to be double the size of the damage