May 14, 2004 32 Replies

Not those that are specific to a particular trade. There, they use the size and type of rod that is used in actual practice.

JTMcC.

That is true. In Seattle the major employers of stick weldors are the shipyards. They all run small rod in multiple passes for lower distortion. A program that concentrated on heavy machine repair would need larger rod.

Unfortunately I don't know of any in the Seattle area.

Skipping school, I decide to respond to what Ernie Leimkuhler fosted Mon, 17 May 2004 01:08:05 GMT in rec.crafts.metalworking , viz:

Check w/ Renton Technical College. I don't know the rep of the welding shop - I just had them fix a "booboo" I made in the machine shop program. (Did you know that 1/16th x 6 inch slit saws are really flexible, and if one side is dull, it cuts to the sharp side if you try too deep a cut? I didn't either, but I do now.) But I see some rather large "chunks" in their recycle bin.

I called around today and got some takers.

I had 3 groups in this evening. One was from Green River College, and the otehr 2 were artist/sculpturs.

I have the guys from Lake Washington Tech coming down Tuesday or Wednesday. Renton Tech said they didn't need any since they got a pile of rod from the Todd Ship yards

What I have left is 1000 lbs each of 8018 and 9018 in 5/32" and 3/32". Another 1000 lbs each of 3/16" 6010 and 7010, and 1000 lbs of 7/32"

7014.

We have definitely put a dent in the pallets of rod.

Thanks to you all.

Sigh....

Gunner

That rifle hanging on the wall of the working-class flat or labourer's cottage is the symbol of democracy. It is our job to see that it stays there. - George Orwell

Olympic college said yes, two friends said no. See you tomorrow or if not you then someone.

Dan

Guess I missed out on the smaller stuff. Damn. I need to keep up on this NG better.

Lane

3/32" rod is pretty usable at home, Lane. 8018 is said to be "like 7018 only a little smoother and stronger". At this price (a little gas money) your risk/return ratio is very favorable indeed. If you ever run 7018 stick go grab a few cans of 8018 and if you like it you've made out like a bandit.

Grant

Thanks Grant. I'm fairly new to electrode welding as I've got a TIG (Syncro

250). I'll email Ernie and get some.

Lane.

I found a whole pallet full under the big 6010.

Olympic College thanks you and Roger. I dropped off about 1300 lbs there this morning. And told Chris Hobson that there was still lots left. He may call and see about getting some more.

Dan

--Figures. I was there yesterday. Woulda stopped and said hello but maybe you heard about the little mishap on the Diamond Princess? Heh.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required