I have an oil pan and intake manifold I would like to get polished. they both are made out of aluminum so what is a ball park price I should expect to see.
Thanks
Ryan
I have an oil pan and intake manifold I would like to get polished. they both are made out of aluminum so what is a ball park price I should expect to see.
Thanks
Ryan
"Steve B" fired this volley in news:jsqrpl$irm$1 @speranza.aioe.org:
The basic rule for polishing is: Use progressively finer abrasives, each being selected to easily take out the scratches from the last. If you don't have any serious "grinding" to do, a lamb's wool buffer starting out with coarse rubbing compound, and working to ultra-fine, should do it. (different pad for each compound).